MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chemours Teflon® PFA Grade 345T Extrusion and Molding Resin for High Temperature Applications  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA)

Material Notes: Teflon® PFA345T us a special-purpose resin available in clear, 2.5mm (0.1in) pellets. This resin is a chemically modified form of Teflon® PFA 345 that combines many of the benefits of the parent resin with several new ones. Like Teflon® PFA345, it offers great flex life and resistance to environmental stress cracking. The additional benefits are improves thermal stability and color while processing.

The improved thermal stability of Teflon® PFA 345T results in reduced amounts of bubbles in final parts and decreased corrosion of processing equipment. This resin can be processed at higher temperatures and higher rated than Teflon® PFA345. Teflon® PFA345T combines the processing ease of conventional thermoplastics with properties similar to those of polytetrafluoroethylene. Properly processed products made from Teflon® PFA345T resin provides the superior properties typical to fluoropolymer resins: retention of physical properties at -196°C (-320°F), and chemical inertness to nearly all industrial chemicals and solvents. Dielectric properties are excellent. Molded products have moderate stiffness and high ultimate elongation.

In a flame situation, products of Teflon® PFA345T resist ignition and no not themselves promote flame spread. When ignited by flame from other sources, the contribution of heat is very small and added at a low rate with very little smoke

Applications

Applications for Teflon® PFA345T include tubing, unsupported pipe linings for production of corrosive chemicals, and wire and cable insulation for chemical environments.

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Fluoroproducts, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.12 - 2.17 g/cc2.12 - 2.17 g/ccASTM D792
Water Absorption <= 0.010 %<= 0.010 %24 hours; ASTM D570
Melt Flow 5.0 g/10 min5.0 g/10 minASTM D3307
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5555ASTM D2240
Tensile Strength, Ultimate 26.2 MPa3800 psiASTM D3307
 9.60 MPa
@Temperature 250 °C
1390 psi
@Temperature 482 °F
ASTM D3307
Tensile Strength, Yield 26.2 MPa3800 psiASTM D3307
Elongation at Break 320 %320 %ASTM D3307
 480 %
@Temperature 250 °C
480 %
@Temperature 482 °F
ASTM D3307
Flexural Modulus 0.551 GPa79.9 ksiASTM D790
Izod Impact, Notched NBNBASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmASTM D257
Surface Resistivity per Square >= 1.00e+17 ohm>= 1.00e+17 ohmASTM D257
Dielectric Constant 2.1
@Frequency 60.0 - 1.00e+6 Hz
2.1
@Frequency 60.0 - 1.00e+6 Hz
ASTM D150
Dielectric Strength 52.0 kV/mm1320 kV/inASTM D149
Dissipation Factor 0.00010
@Frequency 1e+6 Hz
0.00010
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance >= 180 sec>= 180 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear 130 µm/m-°C
@Temperature 21.0 - 100 °C
72.2 µin/in-°F
@Temperature 69.8 - 212 °F
ASTM D696
Melting Point 302 - 310 °C576 - 590 °FASTM D3418
Maximum Service Temperature, Air 260 °C500 °F
Flammability, UL94 V-0V-0
Oxygen Index >= 95 %>= 95 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Processing Temperature 379 - 399 °C714 - 750 °FCure Temperature
 
Descriptive Properties
20% Hydrochloric Acid Transmission, g/100sq in.<0.02
50% Sodium Hydroxide Transmission, g/100sq in.<.02
Acetic Acid Transmission, g/100sq in.0.41
Acetone Transmission, g/100sq in.0.95
Acetophenone Transmission, g/100sq in.0.5
Benzene Transmission, g/100sq in.0.64
Carbon Tetrachloride Transmission, g/100sq in.0.31
Chemical/Solvent ResistanceExcellent
Ethyl Acetate Transmission, g/100sq in.0.76
Folding Endurance, # cycles, .18-.20 mm10-500 E3
Heat of Combustion J/g5300ASTM D240
Hexane Transmission, g/100sq in.0.56
Piperidine Transmission, g/100sq in.0.04
Red Fuming Nitric Acid Transmission, g/100sq in.7.5-1.4
Salt Spray Resistance on aluminum, Hours1000
Sulfuric Acid Transmission, g/100sq in.0.00001
Water Transmission, g/100sq in.0.4
Weather Resistance10Years unaffected in Florida Exposure

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chemours Teflon® PFA Grade 345 Extrusion and Molding Resin
Chemours Teflon® PFA Grade 450 HP Extrusion and Molding Resin
Chemours Teflon® PFA Grade 940 HP Plus Extrusion and Molding Resin
Chemours Teflon® PFA Grade 950 HP Plus Extrusion and Molding Resin
Chemours Teflon® PFA Grade 440 HP Extrusion and Molding Resin

PDU9222 / 33335

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.