MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Saint-Gobain Rulon® 641 Bearing/Seal PTFE
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of friction, and excellent abrasion and corrosion resistance while running without lubrication. They are used in bearing and seal applications from temperature extremes of 400°F to over 500°F with and without additional lubricants. A unique property of Rulon® is the absence of stick slip, that is, erratic low-speed motion. PTFE = polytetrafluoroethylene

641 Grade Bearing/Seal PTFE: FDA compliant, this formulation was specifically developed for food and drug applications. Rulon 641 is designed to run dry without any external lubrication and is compatible with 303 and 316 stainless steel mating surfaces. Rulon 641's high temperature and low wear properties offer major advantages as compared to other competitive FDA bearing materials, such as UHMWPE (Limited temperature tolerance and low load capacity at elevated temperatures) and virgin PTFE (Unacceptable wear properties and low load capacity at elevated temperatures). Rulon 641 is available in standard bearing sizes from 1/8" to 3" ID's White in color.

Suitable for use in environments of steam, wet, dry, vacuum, or FDA type. Mating surface of 25 Rc or harder Steel. Material has electrical and thermal insulation properties. Markets for 641 grade include Appliances, Automotive, Dairy/Food/Beverage, Industrial, Medical, Transportation.
Information provided by Saint Gobain Performance Products.

Vendors: TriStar Plastics Corp. provides engineering, custom fabrication and manufacturing of high-performance plastics and self-lubricating bearing materials, such as Rulon, PEEK, Torlon, CJ Composites and Ultracomp. Capabilities include component design, material selection, prototype and production, manufacturing and surface modification. Call (800) TRI-STAR (800) 874-7827 or visit or www.TStar.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.20 g/cc0.0795 lb/in³ASTM D792
Water Absorption 0.00 %
@Time 86400 sec
0.00 %
@Time 24.0 hour
ASTM D570
Deformation 4.0 %
@Pressure 10.3 MPa
4.0 %
@Pressure 1500 psi
ASTM D621
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 60 - 7060 - 70ASTM D4894
Tensile Strength 21.4 MPa3100 psiASTM D4894
Elongation at Break 350 %350 %ASTM D4894
Flexural Yield Strength 4.20 MPa
@Strain 1 %
609 psi
@Strain 1 %
ASTM D790
Flexural Modulus 0.410 GPa59.5 ksiASTM D790
Compressive Yield Strength 4.60 MPa
@Strain 1 %
667 psi
@Strain 1 %
ASTM D695
Compressive Modulus 0.480 GPa69.6 ksiASTM D695
Coefficient of Friction 0.10 - 0.300.10 - 0.30
Limiting Pressure Velocity 0.350 MPa-m/sec10000 psi-ft/min
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  103 µm/m-°C
@Temperature 37.8 °C
57.2 µin/in-°F
@Temperature 100 °F
 139 µm/m-°C
@Temperature 37.8 °C
77.2 µin/in-°F
@Temperature 100 °F
CTE, linear, Transverse to Flow  76.9 µm/m-°C
@Temperature 149 °C
42.7 µin/in-°F
@Temperature 300 °F
 102 µm/m-°C
@Temperature 149 °C
56.7 µin/in-°F
@Temperature 300 °F
Thermal Conductivity 0.375 W/m-K2.60 BTU-in/hr-ft²-°FASTM D2214
Maximum Service Temperature, Air 288 °C550 °F
Minimum Service Temperature, Air -240 °C-400 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain Rulon® J Bearing/Seal PTFE
Ampco Metal AMPCO® 18 Aluminum Bronze, Extruded and Drawn Rods, 12.7 - 25.4 mm.
Saint-Gobain Rulon® LR Bearing/Seal PTFE
Saint-Gobain Rulon® W2 Bearing/Seal PTFE
Saint-Gobain Rulon® XL Bearing/Seal PTFE

PSTGQZ174 / 68688

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.