MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Refractory Metals

CMW® THERMKON® 83 Tungsten Copper parts  (discontinued **)
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Refractory Metal; Tungsten Alloy

Material Notes: For matching CTE of semiconductor substrates while allowing high thermal transfer.

Information provided by CMW Inc.

1

Vendors: PLANSEE SE: Whether it's high temperatures, aggressive chemicals or extreme mechanical loading: PLANSEE supplies a suitable product solution in refractory metals or composite materials. As the world market leader in powder metallurgically produced high performance materials we combine outstanding materials knowledge with profound applications and technology know-how. Visit us at www.plansee.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 14.84 g/cc0.5361 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 9898
Tensile Strength, Ultimate 690 MPa100000 psi
Tensile Strength, Yield 524 MPa76000 psi
Modulus of Elasticity 234 GPa33900 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000383 ohm-cm0.00000383 ohm-cm(45% IACS)
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.50 µm/m-°C
@Temperature 20.0 °C
4.72 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.192 J/g-°C0.0459 BTU/lb-°F
Thermal Conductivity 220 W/m-K1530 BTU-in/hr-ft²-°F
Melting Point 1080 - 3410 °C1980 - 6170 °F
Solidus 1080 °C1980 °F
Liquidus 3410 °C6170 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 25 %25 %
Tungsten, W 75 %75 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CMW® THERMKON® 62 Tungsten Copper parts
Phosphorus deoxidized tellurium bearing Copper, UNS C14500, H04 Temper 13 mm and 25 mm rods
CMW® ELKONITE® 50W3 Tungsten Copper material ASTM B702
CMW® THERMKON® 68 Tungsten Copper parts
NAECO® ELKON® R45 Copper Tungsten RWMA Class 10

NCMW65 / 15984

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.