MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CHT Group QSil 553 QSI Quantum Silicones Silicone Potting Material
Categories: Polymer; Thermoset; Silicone

Material Notes: QSil 553 is a 100% silicone solids elastomer designed for electronic potting applications. The two-component system offers a flame retardant, thermally conductive, low modulus material that is readily repairable.

Key Features:

  • 100% solids - no solvents
  • Long pot life
  • Good elongation
  • Low modulus
  • Material is UL listed.
Part of the Amber Chemical Group. Data provided by manufacturer.

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.63 g/cc1.63 g/cc"B" component
 1.63 g/cc1.63 g/cc"A" component
Viscosity 6000 cP6000 cP"B" component
 6000 cP6000 cP"A" component
Storage Temperature <= 38.0 °C<= 100 °F12 months
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4545cured 15 mins @ 150°C
Tensile Strength 1.72 MPa249 psicured 15 mins @ 150°C
Elongation at Break 240 %240 %cured 15 mins @ 150°C
100% Modulus 1.24 MPa
@Strain 100 %
180 psi
@Strain 100 %
cured 15 mins @ 150°C
Tear Strength 7.89 kN/m45.0 plicured 15 mins @ 150°C
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.02e+14 ohm-cm4.02e+14 ohm-cm
Dielectric Constant 3.1
@Frequency 1000 Hz
3.1
@Frequency 1000 Hz
Dissipation Factor 0.00900.0090
Comparative Tracking Index 600 V600 V
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.680 W/m-K4.72 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 240 °C464 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Flammability, UL94 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Pot Life 100 min100 min
 
Descriptive Properties
ColorBeige"A" component
 Black"B" component

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CHT Group QSil 551 QSI Quantum Silicones Silicone Potting Material
CHT Group QSil 216 QSI Quantum Silicones Transparent Liquid Silicone Rubber
CHT Group QSil 430 QSI Quantum Silicones Silicone Potting Material
CHT Group QSil 550 QSI Quantum Silicones Silicone Potting Material
CHT Group QSil 550R QSI Quantum Silicones Silicone Potting Material

PACC034 / 22161

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.