MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik Vestodur® 2000 Medium Viscosity PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: Description: Degussa AG’s High Performance Polymers Business Unit manufactures a range of polybutylene terephthalate compounds that are supplied under the registered trademark VESTODUR® . Material properties characterizing VESTODUR compounds are:
  • high thermostability
  • high stiffness
  • low water absorption resulting in high dimensional stability
  • high hardness
  • good strength
  • good sliding friction behavior, low abrasion
  • good creep behavior
  • good electrical properties
  • good chemical resistance
  • good weathering resistance
  • good processability
  • no tendency to form stress cracks

Specific Notes for this Material: Low- to- high-viscosity base types for injection molding applications (e.g., headlight housings, parts in medical technology) and extrusion applications (fiber optic jacketing)

Information provided by degussa.

Evonik Industries is the successor company to Degussa.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.31 g/cc0.0473 lb/in³ISO 1183
Water Absorption at Saturation 0.45 %0.45 %ISO 62
Linear Mold Shrinkage 0.016 cm/cm0.016 in/inPigmentation can change mold shrinkage.
Linear Mold Shrinkage, Transverse 0.016 cm/cm0.016 in/inPigmentation can change mold shrinkage.
Melt Flow 18.34 g/10 min
@Load 2.16 kg,
Temperature 250 °C
18.34 g/10 min
@Load 4.76 lb,
Temperature 482 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7777ISO 868
Ball Indentation Hardness 150 MPa21800 psiH30; ISO 2039-1
Tensile Strength, Yield 55.0 MPa7980 psi50 mm/min; ISO 527-1/2
Elongation at Break >= 50 %>= 50 %50 mm/min; ISO 527-1/2
Elongation at Yield 7.0 %7.0 %50 mm/min; ISO 527-1/2
Tensile Modulus 2.60 GPa377 ksiISO 527-1/2
Charpy Impact Unnotched  30.0 J/cm²
@Temperature -30.0 °C
143 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Constant  3.3
@Frequency 100 Hz
3.3
@Frequency 100 Hz
IEC 60250
 3.5
@Frequency 1e+6 Hz
3.5
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 27.0 kV/mm686 kV/inK20/P50; IEC 60243-1
Dissipation Factor  0.0020
@Frequency 100 Hz
0.0020
@Frequency 100 Hz
IEC 60250
 0.023
@Frequency 1e+6 Hz
0.023
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 575 V575 VTest Solution A, 100 drops; IEC 60112
 600 V600 VTest Solution A, CTI; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 110 µm/m-°C
@Temperature 23.0 - 55.0 °C
61.1 µin/in-°F
@Temperature 73.4 - 131 °F
Longitudinal; ISO 11359
CTE, linear, Transverse to Flow 110 µm/m-°C
@Temperature 23.0 - 55.0 °C
61.1 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359
Melting Point 221 - 226 °C430 - 439 °FDSC
Deflection Temperature at 0.46 MPa (66 psi) 150 °C302 °FISO 75-1/2
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C131 °FISO 75-1/2
Vicat Softening Point 180 °C356 °F50N; ISO 306
 220 °C428 °F10N; ISO 306
Flammability, UL94  HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Oxygen Index 23 %23 %ISO 4589
Glow Wire Test 850 °C
@Thickness 2.00 mm
1560 °F
@Thickness 0.0787 in
IEC 60695-2-1/0-3
 
Descriptive Properties
Electrolytic CorrosionA1 StepIEC 60426

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Gravi-Tech™ GRV-PS-027-BA-WHT Polybutylene Terephthalate (PBT)
Aclo Accucomp Polycarbonate POL051L Medium Viscosity
Celanese Celanex® 1400A PBT, Unfilled
Mitsubishi Xantar® 24 R Polycarbonate
Adell DS-10 General Purpose Polycarbonate

PHUMA04 / 47518

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.