MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Desmomelt® 540/1 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characterization: Desmomelt® 540/1 is a flexible polyurethane with a very high rate of crystallization and very low thermoplasticity. Extruded flat products made from this raw material (hot melt adhesive films and fleeces) are of high quality. Desmomelt® 540/1 has outstanding adhesion on a large number of materials. It has high initial bond strength and thermal stability.

Properties / Applications Desmomelt® 540/1 is suitable for the manufacture of adhesive films and fleeces for bonding many different materials, e.g. leather, textiles, wood fibreboard, various plastics including polyurethane elastomers and flexible PVC.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccDIN 53 479
Viscosity 100 - 500 cP100 - 500 cPSolution viscosity, 15 % in butanone-2 (MEK) at 23 °C Haake RV 12/20 MV-DIN alternative Brookfield LVF; ISO 3219
 
Descriptive Properties
Content<0.1Hydroxyl, DIN 53 240
Crystallization10 minDIN 53 505
Heat resistance80°CASTM D 816

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CENTROPLAST BC NF Organic Thermoplastic, 15% Natural Fiber
Ipiranga Petrochem LB 0216 LLDP
Ipiranga Petrochem LB 0117 LLDP
GEHR Plastics ECO-GEHR® PLA-LF Polylactic Acid
Daelim H&L Plavis-G15 CM 15% Graphite Filled Aromatic Polyimide Bearing

PCOVEST0680 / 202463

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.