MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plaskolite West Optix® CP - 51 General Purpose Acrylic Resin
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, General Purpose, Molded; Acrylic, Optical Grade, Molded

Material Notes: Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are available.

Information provided by Plaskolite West, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ASTM D-792
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm0.0020 - 0.0060 in/inASTM D-955
Melt Flow 14 g/10 min
@Load 3.80 kg,
Temperature 230 °C
14 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D-1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 55.8 MPa8100 psiASTM D-638
Elongation at Break 2.6 %2.6 %ASTM D-638
Modulus of Elasticity 2.89 GPa419 ksiASTM D-638
Flexural Strength 102 MPa14800 psiASTM D-790
Izod Impact, Notched 0.160 J/cm
@Thickness 6.35 mm
0.300 ft-lb/in
@Thickness 0.250 in
ASTM D-256
Gardner Impact 0.226 J
@Thickness 3.17 mm
0.167 ft-lb
@Thickness 0.125 in
Falling Weight; ASTM D-3029 GB
 
Thermal PropertiesMetricEnglishComments
CTE, linear 60.0 µm/m-°C33.3 µin/in-°FASTM D-696
Maximum Service Temperature, Air 85.0 °C185 °FUL-746 ABC
Deflection Temperature at 1.8 MPa (264 psi) 75.6 °C168 °FASTM D-648
Vicat Softening Point 93.9 °C201 °FASTM D-1525
Flammability, UL94 HBHB
 
Optical PropertiesMetricEnglishComments
Haze <= 1.0 %<= 1.0 %ASTM D-1003
Transmission, Visible 92 %92 %ASTM D-1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo Plexiglas® V920 Acrylic
Plaskolite West Optix® CA-41 General Purpose Acrylic Resin
Plaskolite Optix® CP - 51 General Purpose Acrylic Resin

PCONT027 / 150584

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.