MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Eurofoam Evacell EVA 100 EVA + PE Foam
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Polyethylene (PE)

Material Notes: Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, dielectric properties and good insulating properties. It is resistant to UVA radiation. It can be silk-screened and thermoformed.

Information provided by Eurofoam s.r.l.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0800 - 0.100 g/cc0.00289 - 0.00361 lb/in³ISO 845-88
Water Absorption <= 3.0 %<= 3.0 %ASTM D 1056
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore OO 70 - 8070 - 80ASTM D 2240
Tensile Strength 1.30 MPa189 psiASTM D 412
Elongation at Break >= 130 %>= 130 %ASTM D 412
Compressive Yield Strength 0.0900 MPa
@Strain 25 %
13.1 psi
@Strain 25 %
ASTM 1056/85
Tear Strength 0.330 kN/m1.88 pliASTM D 624
Compression Set 10 %
@Strain 25 %
10 %
@Strain 25 %
ASTM D 395
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 70.0 °C158 °FASTM D 3575
Minimum Service Temperature, Air -10.0 °C14.0 °FASTM D 3575
 
Descriptive Properties
Cellular StructureClosed
Declaration of Heavy Metal AbsenceConformRoHS2002/95/EC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eurofoam Evacell EVA 30 EVA + PE Foam
Braskem VA2019A EVA Foam Copolymer
Eurofoam Evacell EVA 200 EVA + PE Foam
Eurofoam Evacell EVA 50/S EVA + NR Foam
Eurofoam Evacell XM 2001 EVA + PE Foam

PEUROF928 / 157191

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.