MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Huntsman IROGRAN® A 87 P 4946 TPU-Polyester
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Introduction: IROGRAN A 87 P 4946 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 87 P 4946 is part of the HUNTSMAN technical extrusion product range and offers a specially designed, flexible material with high extrudability.

Performance Features:

  • High microbial resistance
  • Excellent hydrolysis resistance
  • High stability of melt
  • High production rate

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³Injection molded parts; ASTM D792
Linear Mold Shrinkage 0.0080 cm/cm0.0080 in/inInjection molded; ASTM D955
Melt Index of Compound 65 g/10 min
@Load 21.6 kg,
Temperature 190 °C
65 g/10 min
@Load 47.6 lb,
Temperature 374 °F
MVR, [cm3/10 min]
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8787Injection molded parts; ASTM D2240
Hardness, Shore D 3838Injection molded parts; ASTM D2240
Tensile Strength at Break 40.0 MPa5800 psiInjection molded parts; DIN 53504
Elongation at Break 650 %650 %Injection molded parts; DIN 53504
100% Modulus 7.00 MPa
@Strain 100 %
1020 psi
@Strain 100 %
Injection molded parts; DIN 53504
300% Modulus 11.0 MPa
@Strain 300 %
1600 psi
@Strain 300 %
Injection molded parts; DIN 53504
Tear Strength 98.2 kN/m560 pliInjection molded parts; ASTM D624
Abrasion 3535mm3, Injection molded; ISO 4649
 
Processing PropertiesMetricEnglishComments
Feed Temperature 25.0 - 35.0 °C77.0 - 95.0 °FInjection
 25.0 - 40.0 °C77.0 - 104 °FExtrusion
Middle Barrel Temperature 175 - 185 °C347 - 365 °FExtrusion
Nozzle Temperature 180 - 190 °C356 - 374 °FExtrusion
 185 - 200 °C365 - 392 °FInjection
Adapter Temperature 185 - 195 °C365 - 383 °FExtrusion
Die Temperature 185 - 195 °C365 - 383 °FExtrusion
Mold Temperature 20.0 - 50.0 °C68.0 - 122 °FInjection
 
Descriptive Properties
Heating Zone185-195°CInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman PE7076 Profile Extrusion Polyethylene
Borealis Bormed™ LE6609-PH LDPE for Pharmaceutical Blow Molding
Lubrizol Advanced Materials PEARLTHANE® 11T93 Thermoplastic Polyurethane Elastomer
Lubrizol Estane® S190A Thermoplastic Polyurethane
Barlog Plastics KEBAFLEX U A 85 HT B01 natural TPU, Shore A85, natural, high temperature resistance

PHUQ104 / 159477

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.