MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total 3289MZ Polypropylene, Homopolymer Sheet Extrusion and Thermoforming Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: ATOFINA 3289MZ produces thermoformed parts with superior clarity, side wall stiffness and gloss. 3289MZ contains an antistatic agent that will help protect thermoformed parts from shelf dusting and enhance part stacking. 3289MZ features minimum taste and odor and optimum thermal stability for superior color and processability. 3289MZ complies with all applicable FDA regulations and may be used under these provisions for food contact and packaging.

Applications: ATOFINA 3289MZ is ideal for del containers, drinking cups, lids, and food service trays.

Information provided provided by Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.905 g/cc0.0327 lb/in³ASTM D1505
Moisture Vapor Transmission 0.177 cc-mm/m²-24hr-atm0.450 cc-mil/100 in²-24hr-atmASTM E96
Oxygen Transmission 94.5 cc-mm/m²-24hr-atm240 cc-mil/100 in²-24hr-atmASTM D1434
Melt Flow 1.8 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1.8 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 35.9 MPa5200 psiASTM D638
Elongation at Break 10 %10 %ASTM D882
Tensile Modulus 1.65 GPa240 ksiASTM D882
Flexural Modulus 1.45 GPa210 ksiASTM D 790
Izod Impact, Notched 0.400 J/cm0.749 ft-lb/inASTM D256A
 
Thermal PropertiesMetricEnglishComments
Melting Point 165 °C329 °FDSC-2 Differential Scanning Calorimeter
Deflection Temperature at 0.46 MPa (66 psi) 115 °C239 °FASTM D648
 
Optical PropertiesMetricEnglishComments
Haze 1.0 %1.0 %ASTM D1003

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total 3289M Polypropylene, Thermoforming Grade
Total 6289MZ Polypropylene, Thermoforming Grade
Formosa Plastics Formolene® 4142K Extrusion - Sheet - Thermoforming Polypropylene
Overview of materials for Polypropylene, Extrusion Grade
Total 7253X Polypropylene, Random Copolymer Extrusion Grade

PFINAA061 / 38497

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.