MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis FT5232 Low Density Polyethylene  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: FT5232 is a Low Density Polyethylene for Film Extrusion. Tubular Technology. Includes medium slip additive and antioxidant. This grade is developed for the production of packaging film with good optical properties for medium duty film applications. Applications FT5232 has been developed especially for applications like: carrier-bag film, pouches, lamination films, and food packaging.

Information provided by Borealis AG

Key Words: LDPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.923 g/cc0.0333 lb/in³ISO 1183
Melt Flow 0.75 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.75 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Slip Level 550 ppm550 ppmerucamide; Borealis Method
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 250 %250 %ISO 527-3
Film Elongation at Break, TD 550 %550 %ISO 527-3
Tensile Modulus 0.230 GPa33.4 ksiMD; ASTM D882-A
 0.260 GPa37.7 ksiTD; ASTM D882-A
Puncture Energy 2.50 J1.84 ft-lb66N; ASTM D5748
Coefficient of Friction, Dynamic 0.400.40ISO 8295
Elmendorf Tear Strength, MD 10.19 g/micron258.8 g/milISO 6383/2
Elmendorf Tear Strength, TD 5.097 g/micron129.5 g/milISO 6383/2
Dart Drop Test 120 g
@Thickness 0.0400 mm
0.265 lb
@Thickness 0.00157 in
ISO 7765-1
Film Tensile Strength at Break, MD 27.0 MPa3920 psiISO 527-3
Film Tensile Strength at Break, TD 24.0 MPa3480 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 112 °C234 °FISO 11357-3
Vicat Softening Point 97.0 °C207 °FISO 306
 
Optical PropertiesMetricEnglishComments
Haze 8.0 %8.0 %ASTM D1003
Gloss 85 %85 %ASTM D2457

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis FT5231 Low Density Polyethylene
Borealis FT5230 Low Density Polyethylene
Borealis FG5224 Linear Low Density Polyethylene
Borealis HD234CF Polypropylene
Borealis FT5236 Low Density Polyethylene

PBOREA455 / 108714

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.