MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco AREMCOLOX™ 502-1600 (94%) Machinable Boron Nitride 94%  (discontinued **)
Categories: Ceramic; Machinable Ceramic; Nitride

Material Notes: Hot-pressed 94% boron nitride. High thermal conductivity. Easily machined. Non-reactive in molten salts, aluminum and other metals. Plates from 1/4" to 1" thick; rods from 1/4" to 3" diameter; bars from 1/4" x 1/4" to 2"x 2".

Vendors: Aremco offers a range of machinable ceramics. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.90 g/cc1.90 g/cc
Porosity 11 %11 %
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 51.7 MPa7500 psi
Compressive Strength 68.9 MPa10000 psi
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 4.1
@Frequency 1e+6 Hz
4.1
@Frequency 1e+6 Hz
Dielectric Strength 52.8 kV/mm1340 kV/in
Dissipation Factor <= 0.00020
@Frequency 1e+6 Hz
<= 0.00020
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 3.96 µm/m-°C
@Temperature 20.0 °C
2.20 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 55.00 W/m-K381.7 BTU-in/hr-ft²-°F
Maximum Service Temperature, Inert 1150 °C2100 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aremco AREMCOLOX™ 502-1550 (Med. Density) Machinable Zirconium Phosphate
Aremco AREMCOLOX™ 502-1600 (99%) Machinable Boron Nitride 99%
Aremco AREMCOLOX™ 502-600 Machinable Glass Ceramic
Corning Macor® Machinable Glass Ceramic
Crystex Composites Mykroy/Mycalex MM 400 Machining Grade Glass-bonded Mica Composite

ZCAREM09 / 550

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.