MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CIMBAR CIMBAR™ BF Barite Powder (BaSO4)
Categories: Ceramic; Other Engineering Material; Additive/Filler for Polymer

Material Notes: CIMBAR Performance Minerals BF product is the next generation of precipitated extenders. With its micro-fine particle size, high barium sulfate content, low solubility, high brightness and chemical inertness, BF is ideal for applications such as topcoats, printing inks, powder coatings and lead-acid batteries as well as many others. Cimbar BF has excellent gloss, dispersability and weather resistance.

Uses:

  • Plastics
  • Architectural coatings
  • Batteries
  • Cosmetics
  • Pharmaceuticals
  • Automotive Primers
  • Automotive Topcoats
  • Gloss Enamels
  • Powder Coatings
  • Semi-gloss Latexes
  • Industrial Coatings

Information provided by Cimbar Performance Minerals.

Key Words: BaSO4, Baryte, Barium Sulfate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 4.40 g/cc4.40 g/cc
Fineness 8.08.0Hegman Fineness
Particle Size 0.68 µm0.68 µmmean
pH 8.08.0
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 3.03.0
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.641.64
 
Descriptive Properties
BaSO4 (%)99
Color-a-0.32
Color-b0.84
Color-L99.3
Color-Z97.3
Paint Coating Gloss (20/60)59.0/89.8
Paint Viscosity (10/100)1010/530

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CIMBAR BARIMITE™ XF High Purity Barite (BaSO4)
CIMBAR BARIMITE™ UF High Purity Barite (BaSO4)
CIMBAR BARIMITE™ NO. 22 Barites High Purity Barite (BaSO4)
CIMBAR BARIMITE™ G-50 High Purity Barite (BaSO4)
CIMBAR BARIMITE™ 200 High Purity Barite (BaSO4)

CIMBAR907 / 133389

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.