MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Lupranate® MI Isocyanate
Categories: Fluid

Material Notes: Description: Lupranate® MI Isocyanate is pure diphenylmethane diisocyanate containing a higher amount of 2,4´ isomer than Lupranate M Isocyanate or Lupranate MS Isocyanate. Lupranate MI Isocyanate has a functionality of 2.0 and is liquid at room temperature. Lupranate MI isocyanate is used in the isocyanate component for the preparation of flexible, semi-flexible and microcellular urethane foams. Lupranate MI Isocyanate can also be used for the production of adhesives, coatings and sealants

Information provided by BASF

Key Words: 2,4' Diphenylmethane Diisocyanate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³
Vapor Pressure 4.00e-7 bar
@Temperature 25.0 °C
0.000300 torr
@Temperature 77.0 °F
 
Thermal PropertiesMetricEnglishComments
Melting Point 10.0 - 15.0 °C50.0 - 59.0 °FFreezing Point
Boiling Point >= 190 °C
@Pressure 0.000667 MPa
>= 374 °F
@Pressure 0.0967 psi
Flash Point 199 °C390 °F
 
Descriptive Properties
ColorColorless to Reddish Yellow
Composition2,4' Isomer0.5
 Hydrolyzable Chlorine<400 ppm
 NCO content0.335
Purity99.5 percent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Lupranate® 5143 Isocyanate
BASF Lupranate® M70L Isocyanate
BASF Lupranate® MP102 Isocyanate Modified MDI
BASF Lupranate® 277 Isocyanate
BASF Lupragen® N 201 TEDA in DPG

PBASG0697 / 132330

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.