MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chevron Phillips Marlex® HXM 50100-01 Extra high molecular weight hexene copolymer
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: Benefits: excellent balance of stress cracking resistance, good melt strength, excellent stress cracking resistance, good rigidity, excellent impact strength even at low temperatures

Applications: 55-gallon shipping containers, gasoline tanks, agricultural chemical tanks, pallets, cattle feeders, large formed parts, boats

Information provided by Chevron Phillips Chemical Company

Key Words: UHMWPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.949 g/cc0.0343 lb/in³ASTM D1505
Environmental Stress Crack Resistance >= 600 hour
@Temperature 50.0 °C
>= 600 hour
@Temperature 122 °F
Condition A and Condition B; ASTM D 1693
High Load Melt Index 12 g/10 min
@Load 21.6 kg,
Temperature 190 °C
12 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 25.0 MPa3630 psiASTM D638 Type IV
Elongation at Break >= 600 %>= 600 %ASTM D638 Type IV
Flexural Modulus 1.20 GPa174 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -91.0 °C<= -132 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Processing Temperature 154 - 182 °C309 - 360 °FThermoforming Surface
 188 - 232 °C370 - 450 °FBlow Molding
 232 - 268 °C450 - 514 °FExtrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® HXM 50100 Extra high molecular weight hexene copolymer
Westlake Plastics Lennite® Biocompatible Implant Grade UHMW-PE
Chevron Phillips Marlex® HXM 50100-02 Extra high molecular weight hexene copolymer
Polikim ULPOLEN® 1000 UHMWPE Standard
Chevron Phillips Marlex® HXB TR-512 Extra high molecular weight polyethylene

PCHEVM02 / 20293

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.