MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LNP Lubriloy® Z- BK8-950 Polyphenylene Ether + Polystyrene, Proprietary Filler  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polystyrene (PS)

Material Notes:
  • Features: Lubricated
  • Forms: Pellets
  • Processing Method: Injection Molding

Information provided by LNP, a GE Plastics Company.

This data sheet is labeled Discontinued; however many LNP grades are still active under new names instituted after the SABIC purchase.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/ccMethod A; ASTM D792
Density 1.04 g/cc0.0376 lb/in³ISO 1183
Linear Mold Shrinkage 0.0080 - 0.0090 cm/cm0.0080 - 0.0090 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.011 cm/cm0.011 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 42.1 MPa6110 psiASTM D638
Tensile Strength, Yield 46.9 MPa6800 psiASTM D638
Elongation at Break 52 %52 %ASTM D638
Elongation at Yield 4.2 %4.2 %ASTM D638
Flexural Strength 68.9 MPa9990 psiASTM D790
Flexural Modulus 2.09 GPa303 ksiASTM D790
Izod Impact, Notched 1.07 J/cm
@Thickness 3.18 mm
2.00 ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 20.3 J/cm
@Thickness 3.18 mm
38.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Notched (ISO) 11.9 kJ/m²5.66 ft-lb/in²ISO 180
Izod Impact, Unnotched (ISO) 173 kJ/m²82.3 ft-lb/in²ISO 180
K (wear) Factor 80.6 x 10-8 mm³/N-M40.0 x 10-10 in³-min/ft-lb-hr40psi, 50ft/min; tested in accordance with LNP WI-0687
 
Thermal PropertiesMetricEnglishComments
CTE, linear 81.0 µm/m-°C
@Temperature 20.0 °C
45.0 µin/in-°F
@Temperature 68.0 °F
TMA; ASTM E831
CTE, linear, Transverse to Flow 88.0 µm/m-°C
@Temperature 20.0 °C
48.9 µin/in-°F
@Temperature 68.0 °F
TMA; ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 141 °C286 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 122 °C252 °FUnannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 277 - 293 °C531 - 559 °F
Mold Temperature 60.0 - 93.3 °C140 - 200 °F
Drying Temperature 82.2 °C180 °F
Dry Time 4 hour4 hour
Back Pressure 0.172 - 0.345 MPa24.9 - 50.0 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Westlake Plastics Norylux™ EN-265 Modified Polyphenylene Oxide
RTP Company RTP 1799 X 138211 C Modified Polyphenylene Oxide (PPO); Glass Fiber - Flame Retardant
RTP Company RTP 1701 Modified Polyphenylene Oxide (PPO), Glass Fiber
Celanese SO.F.TER Norfor® 90 PPE compound

PZLNP1235 / 51317

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.