MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Aearo E-A-R Specialty Composites VersaDamp™ V-2525 TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded into a wide variety of standard or custom isolators, including grommets, equipment mounts, bumpers, and gaskets. They feature high internal damping properties for low amplification at resonance to protect equipment during frequency cycling and random shocks, effective shock protection for sensitive mechanisms within minimum sway parameters, and quick return to equilibrium after vibrations or shocks.

Information provided by Aearo E-A-R Specialty Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 56565 sec.; ASTM D2240
Tensile Strength at Break 4.90 MPa710 psiASTM D412
Elongation at Break 305 %305 %ASTM D412
Tensile Modulus 0.00248 GPa0.360 ksiASTM D412
Compressive Yield Strength 0.140 MPa20.3 psiCompressive Load Deflection at 5%; ASTM D575
 0.370 MPa53.7 psiCompressive Load Deflection at 10%; ASTM D575
 0.590 MPa85.6 psiCompressive Load Deflection at 15%; ASTM D575
 0.850 MPa123 psiCompressive Load Deflection at 20%; ASTM D575
 1.21 MPa175 psiCompressive Load Deflection at 25%; ASTM D575
Compressive Modulus 0.00430 GPa0.624 ksiat 15% Compression; ASTM D575
Rebound 36 %36 %Bashore Rebound; 22°C; ASTM D2632
 51 %51 %Bashore Rebound; 70°C; ASTM D2632
Tear Strength 21.2 kN/m121 pliASTM D624
Compression Set  8.1 %
@Temperature 20.0 °C,
Time 86400 sec
8.1 %
@Temperature 68.0 °F,
Time 24.0 hour
ASTM D395B
 13.4 %
@Temperature 20.0 °C,
Time 1800 sec
13.4 %
@Temperature 68.0 °F,
Time 0.500 hour
ASTM D395B
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 100 °C212 °FContinuous
 125 °C257 °FIntermittent
Brittleness Temperature -66.0 °C-86.8 °FASTM D2137
Glass Transition Temp, Tg -64.0 °C-83.2 °FDMA @ 10 Hz; ASTM D2240
Flammability, UL94 HBHBMeets HBF
 
Descriptive Properties
Bacterial ResistanceMeetsASTM G21
Fungal ResistanceMeetsASTM G22
MVSS 302 FlammabilityPasses
Ozone ResistanceNo CrackingASTM D1149-91
Relative Peak Transmissibility13.3 dBG-411 Grommet; 1.2lb load @ 20°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aearo E-A-R Specialty Composites VersaDamp™ V-2550 TPE
Aearo E-A-R Specialty Composites VersaDamp™ V-2375 TPE
Aearo E-A-R Specialty Composites VersaDamp™ V-2750 TPE
Aearo E-A-R Specialty Composites VersaDamp™ V-2590 TPE
Aearo E-A-R Specialty Composites VersaDamp™ V-2575 TPE

PEARC06 / 35304

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.