MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Bamberger Polymers Bapolene® 350F High Density Polyethylene, Film Extrusion Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Bapolene 350F has superior melt, good processability, bubble stability, and drawdown. This product meets US FDA 21 CFR 177.1520.

Applications: Industrial liners.

Film properties below are based on a flim thickness of 0.5 mil and blow-up ratio of 4:1.

Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers

Key Words: Good Drawdown; Good Processability
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³ASTM D1505
Thickness 25.4 microns1.00 mil
Melt Flow 0.050 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.050 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D-1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 200 %200 %ASTM D-882
Film Elongation at Break, TD 200 %200 %ASTM D-882
Elmendorf Tear Strength MD 10 g10 gASTM D1922
Elmendorf Tear Strength TD 22 g22 gASTM D1922
Dart Drop Test 200 g
@Thickness 0.0254 mm
0.441 lb
@Thickness 0.00100 in
ASTM D1709
Film Tensile Strength at Break, MD 51.7 MPa7500 psiASTM D-882
Film Tensile Strength at Break, TD 28.3 MPa4100 psiASTM D-882
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
processBlown Film

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bamberger Polymers Bapolene® 345F Medium Density Polyethylene, Film Extrusion Grade
Overview of materials for High Density Polyethylene (HDPE), Extruded
Bamberger Polymers Bapolene® 0760 High Density Polyethylene, Blow Molding Grade
Overview of materials for High Density Polyethylene (HDPE), Film Grade
Bamberger Polymers Bapolene® 105F Low Density Polyethylene Film Resin

PBP3B075 / 20796

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.