MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® A 548B V15 PA66, 15% glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 20% Glass Fiber Filled

Material Notes: Description: TECHNYL® A 548B V15 is a copolyamide 6.6/6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.

Benefits: The product offers an excellent long term heat resistance and is suitable to work in environments characterized by a very high temperature.

Available in: Europe

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.

Applications: Thanks to its high melt strength, this product can be used to produce hollow parts, by suction blow molding technology, like tanks or ducts. Typical applications are turbo air ducts, especially inlet ducts up to 200°C.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ISO 1183/A
Linear Mold Shrinkage 0.010 cm/cm0.010 in/inIsotropy
Linear Mold Shrinkage, Flow 0.0098 cm/cm0.0098 in/in
Linear Mold Shrinkage, Transverse 0.0098 cm/cm0.0098 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 100 MPa14500 psiISO 527 Type 1A
Tensile Stress at Strain  30.0 MPa
@Strain 1 %
4350 psi
@Strain 1 %
 85.0 MPa
@Strain 2 %
12300 psi
@Strain 2 %
 90.0 MPa
@Strain 4 %
13100 psi
@Strain 4 %
 92.0 MPa
@Strain 3 %
13300 psi
@Strain 3 %
Elongation at Break 5.0 %5.0 %ISO 527 Type 1A
Tensile Modulus 5.20 GPa754 ksiISO 527 Type 1A
Flexural Strength 130 MPa18900 psiISO 178
Flexural Modulus 4.10 GPa595 ksiISO 178
Izod Impact, Notched (ISO) 13.0 kJ/m²6.19 ft-lb/in²ISO 180/1eA
Izod Impact, Unnotched (ISO) 58.0 kJ/m²27.6 ft-lb/in²ISO 180/1eU
Charpy Impact Unnotched 6.80 J/cm²32.4 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.10 J/cm²5.23 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 242 °C468 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 215 °C419 °FISO 75/Af
 
Processing PropertiesMetricEnglishComments
Feed Temperature 240 - 260 °C464 - 500 °F
Adapter Temperature 245 - 265 °C473 - 509 °F
Die Temperature 250 - 270 °C482 - 518 °F
Head Temperature 250 - 270 °C482 - 518 °F
Screw Cooling Temperature 245 - 265 °C473 - 509 °F
Mold Temperature 40.0 - 60.0 °C104 - 140 °F
Drying Temperature 80.0 °C
@Time 28800 sec
176 °F
@Time 8.00 hour
dew point -35°C
Moisture Content <= 0.080 %<= 0.080 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo Technyl® C216V15 15% Glass Filled Nylon 6
Domo Technyl® C216V25 25% Glass Filled Nylon 6
Domo Technyl® C216V30 30% Glass Filled Nylon 6
Domo TECHNYL® C 216 V30 PA6, 30% glass fiber, DRY
Ashley Polymers Ashlene® 527LD-14G Nylon 66, 14% Glass Reinforced

PRHOD718 / 137949

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.