MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Elvaloy® 3217 AC Ethylene and 17% Butyl Acrylate Copolymer
Categories: Polymer; Film; Thermoplastic; Ethylene Butyl Acrylate

Material Notes: Elvaloy® 3217 AC contains antioxidant, slip and antiblock additives.

Elvaloy® 3217 AC has been developed for film applications requiring a combination of softness, toughness and low friction. Typical applications are hygiene films and examination and veterinary gloves. Flexibility and easy sealing make it suitable for colostomy, ileostomy and urinary pouches.

Processing characteristics of Elvaloy® 3217 AC are similar to LDPE and conventional polyethylene extruders are recommended. Elvaloy® 3217 AC works very well in both hot bar and high frequency welding units. The low seal temperature ensures short welding cycles and little impact on packed content. The high polarity of EBA gives good performance in high frequency welding. The slip and antiblock content is adapted to production of thin films. For thicker films, mixing with Elvaloy® 3117 is recommended to increase friction.

Information provided by DuPont.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.926 g/cc0.0335 lb/in³Base resin; ISO 1183
Thickness 25.0 microns0.984 milMinimum recommended
Melt Flow 1.8 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.8 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238 - ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 240 %240 %500 mm/min; ISO 527-3
Film Elongation at Break, TD 680 %680 %500 mm/min; ISO 527-3
Coefficient of Friction, Dynamic 0.100.10MD; ISO 8295
Film Tensile Strength at Break, MD 25.0 MPa3630 psi500 mm/min; ISO 527-3
Film Tensile Strength at Break, TD 15.0 MPa2180 psi500 mm/min; ISO 527-3
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 150 °C302 °FExtrusion lamination and extrusion coating
 150 °C302 °FCast film
 150 °C302 °FBlown film
Middle Barrel Temperature 160 °C320 °FBlown film
 210 °C410 °FCast film
 220 °C428 °FExtrusion lamination
Front Barrel Temperature 170 °C338 °FBlown film
 250 °C482 °FCast film
 290 °C554 °FExtrusion lamination
Adapter Temperature 180 °C356 °FBlown film
 250 °C482 °FCast Film
 290 °C554 °FExtrusion lamination
Die Temperature 180 °C356 °FBlown film
 250 °C482 °FCast film
 290 °C554 °FExtrusion lamination
Melt Temperature 170 - 180 °C338 - 356 °F
Blow-up Ratio (BUR) 2.02.0for 25 micron film
 
Descriptive Properties
BA-Content17 wt.%DuPont Method
Puncture Resistance18 NDuPont Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Elvaloy® 3117 AC Ethylene and 17% Butyl Acrylate Copolymer
Dow Elvaloy® 3717 AC Ethylene and 17% Butyl Acrylate Copolymer
Dow Elvaloy® 3427 AC Ethylene and 27% Butyl Acrylate Copolymer
Dow Elvaloy® 2112 AC Ethylene and 12% Ethyl Acrylate Copolymer
Dow Elvaloy® 1218 AC Ethylene and 18% Methyl Acrylate Copolymer

PDUPM068 / 33735

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.