MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Teijin Films Mylar® WC Polyester Film, 75 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Mylar® WC films are general-purpose electrical grade films, similar to Mylar® EL. These clear to hazy films are tough and durable as a core wrap. They offer good dielectrics and good handling characteristics.

General Product Info: Mylar® Type WC films combine the tensile strength, dimensional stability, and dielectric strength needed for wire and cable applications.

Typical Applications: Mylar® WC films possess the characteristics required for wire and cable used in the telecommunications and power transmission fields.

Approvals: UL recognized - MIL-I631D, TYPE G and UL 94 VTM-2 - for 92 - 500 gauge (0.023 - 0.13 mm)

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.39 g/cc0.0502 lb/in³Typical Mylar®; ASTM D1505
Thickness 19.0 microns0.750 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 110 %110 %ASTM D882A
Film Elongation at Break, TD 90 %90 %ASTM D882A
Film Tensile Strength at Break, MD 193 MPa28000 psiASTM D882A
Film Tensile Strength at Break, TD 234 MPa34000 psiASTM D882A
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 183.7 kV/mm4667 kV/in1/4" electrode 500 V/sec 25°C in air; ASTM D149
Dielectric Breakdown 3500 V3500 V1/4" electrode 500 V/sec 25°C in air; ASTM D149
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.17 J/g-°C0.280 BTU/lb-°FTypical Mylar®
Melting Point 254 °C489 °FTypical Mylar® via DSC
Shrinkage, MD 2.0 %
@Temperature 150 °C,
Time 1800 sec
2.0 %
@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 1.1 %
@Temperature 150 °C,
Time 1800 sec
1.1 %
@Temperature 302 °F,
Time 0.500 hour
Unrestrained
 
Optical PropertiesMetricEnglishComments
Haze 15 %15 %ASTM D1003
 
Descriptive Properties
Yield (nominal)26500 in2/lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Teijin Films Mylar® A Polyester Film, 75 Gauge
DuPont Teijin Films Mylar® EL Polyester Film, 75 Gauge
DuPont Teijin Films Mylar® OL2 Polyester Film, 75 Gauge
AdvanSix Capran® 1200 Bi-Axially Oriented Nylon Film
DuPont Teijin Films Mylar® E Polyester Film, 48 Gauge

PDTZ9429 / 139746

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.