MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Carlson GOC 276 Nickel-Molybdenum-Chromium
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: General Description

Carlson Alloy GOC 276 is a nickel-molybdenum-chromium alloy exhibiting outstanding corrosion resistance over a wide range of service environments. This alloy is generally use in the as-welded condition. It dies not require a post-weld heat treatment because the low carbon content minimizes the formation of grain boundary precipitates in the heat-affected zones of the weld joints.

High nickel and molybdenum content provides excellent resistance to corrosion in reducing atmospheres.

High chromium content provides excellent resistance to oxidation at temperatures up to 1900°F (1038°C).

GOC 276 also exhibits exceptional resistance to general pitting and stress corrosion cracking.

Applications

GOC 276 is used extensively in severe operating environments, including those encountered in chemical processing, pulp and paper, air pollution control, ore processing, waste treatment and disposal, and other applications. GOC 276 exhibits excellent resistance to ferric and cupric chlorides, hot contaminated organics and inorganics, chlorine, formic acid, acetic acid, acetic anhydride, sea water and brine. It is one of the few alloys that is resistance to wet chlorine gas, hypochlorite, and chlorine dioxide.

  • Chemical Processing Equipment – heat exchangers, reactors and vessels, evaporators, pumps, valves and piping for processing sulfuric acid, pesticides, phenol, styrene, vinyl chloride, chlorine and other chemicals
  • Pulp and Paper – bleaching, head boxes, and waste-gas scrubbers.
  • Air Pollution Control – power plant scrubbers and related equipment, electrostatic precipitators, reheaters, waste-heat recovery systems, industrial boiler scrubbers, marine inert gas scrubbers
  • Ore Processing – uranium and aluminum sulfate
  • Waste Treatment and Disposal – sewage sludge incinerators, industrial and municipal incinerators, chemical and toxic waste incinerators.

Information provided by Carlson

Key Words: UNS N10276
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.89 g/cc0.321 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B <= 100<= 100
Tensile Strength at Break >= 689 MPa>= 100000 psi
Tensile Strength, Yield >= 283 MPa
@Strain 0.2 %
>= 41000 psi
@Strain 0.2 %
Elongation at Break >= 40 %>= 40 %
 
Electrical PropertiesMetricEnglishComments
Magnetic Permeability 1.0011.001B-H at 200H
 
Thermal PropertiesMetricEnglishComments
CTE, linear  12.1 µm/m-°C
@Temperature 23.9 - 204 °C
6.70 µin/in-°F
@Temperature 75.0 - 400 °F
 13.1 µm/m-°C
@Temperature 23.9 - 427 °C
7.30 µin/in-°F
@Temperature 75.0 - 800 °F
 14.0 µm/m-°C
@Temperature 23.9 - 649 °C
7.80 µin/in-°F
@Temperature 75.0 - 1200 °F
 15.8 µm/m-°C
@Temperature 23.9 - 871 °C
8.80 µin/in-°F
@Temperature 75.0 - 1600 °F
Specific Heat Capacity 0.427 J/g-°C0.102 BTU/lb-°F
Melting Point 1324 - 1370 °C2415 - 2500 °F
Solidus 1324 °C2415 °F
Liquidus 1370 °C2500 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.010 %<= 0.010 %
Chromium, Cr 14.5 - 16.5 %14.5 - 16.5 %
Cobalt, Co <= 2.5 %<= 2.5 %
Iron, Fe 4.0 - 7.0 %4.0 - 7.0 %
Manganese, Mn <= 1.0 %<= 1.0 %
Molybdenum, Mo 15 - 17 %15 - 17 %
Nickel, Ni 50.99 - 63.5 %50.99 - 63.5 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si <= 0.080 %<= 0.080 %
Sulfur, S <= 0.030 %<= 0.030 %
Tungsten, W 3.0 - 4.5 %3.0 - 4.5 %
Vanadium, V <= 0.35 %<= 0.35 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Molybdenum TZC (Mo-1Ti-0.3Zr)
W-50Mo Tungsten Alloy
Special Metals INCONEL® Alloy C-276
Ametek Molybdenum-Copper Composite AMC 3169
ATI Allvac® Nickelvac® C-276 UNS N10276 Nickel Superalloy

NCARLSO25 / 15832

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.