MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Phillips 66 Triton® OSP 320 NLGI Grade 2
Categories: Fluid; Lubricant; Calcium Gellant

Material Notes: Phillips 66® Triton OSP 320 is a premium quality, synthetic, extreme-pressure (EP) calcium sulfonate grease specially developed for use in industrial and heavy mobile equipment operating under severe conditions involving high loads, high temperatures and/or high humidity. Triton OSP 320 is manufactured with high-viscosity synthetic base oil, a calcium sulfonate thickener, and select additives to protect against rust and corrosion in high-humidity, high-temperature applications such as those found in the steel and paper industries. It has outstanding resistance to water washout, high load carrying capacity to protect against wear, and outstanding shear stability to resist mechanical breakdown. The synthetic base oil allows its use over a wide temperature range.

Applications:

  • Industrial equipment operating under unfavorable conditions involving water contamination, high loads and/or high temperatures
  • Plain and rolling-element bearings operating in corrosive environmental conditions
  • Steel mill and slab mill roller bearings
  • Marine and heavy mobile equipment exposed to salt water
  • Paper machine wet-and dry-end bearings and hot calendar stacks
Features/Benefits:
  • Excellent oxidation resistance and thermal stability at high temperatures
  • Outstanding rust and corrosion protection, including resistance to saltwater corrosion
  • Excellent extreme-pressure and antiwear properties
  • Outstanding resistance to water washout
  • Outstanding shear stability
  • High dropping point (>550°F)
  • Does not contain heavy metals or other environmentally undesirable components

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measurement 189189Index
Saybolt Viscosity at 100°F 1700 SUS1700 SUS
Saybolt Viscosity at 210°F 212 SUS212 SUS
Kinematic Viscosity at 40°C (104°F) 334 cSt334 cSt
Kinematic Viscosity at 100°C (212°F) 44 cSt44 cSt
Oxidative Stability 100 hour
@Pressure 0.00689 MPa
100 hour
@Pressure 1.00 psi
ASTM D942
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Weld Load 400 kg882 lb (mass)ASTM D2596
Four Ball Wear 0.500 mm0.0197 inScar Diameter; ASTM D2266
Penetration 265 - 295265 - 29560 strokes; ASTM D217
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 190 °C374 °FContinuous
 204 °C399 °FIntermittent
Minimum Service Temperature, Air -34.0 °C-29.2 °F
Dropping Point 300 °C572 °F
 
Descriptive Properties
ColorBlue
ThickenerCalcium Sulfonate
Water Washout Resistance0.02Weight Loss @ 175°F, ASTM D1264

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Phillips 66 Triton® XD5 NGLI Grade 1
Phillips 66 Omniguard® NLGI Grade 1
Phillips 66 Omniguard® 460 NLGI Grade 1
Phillips 66 Kendall® C915 Fifth Wheel Grease NLGI Grade 1
Lubriplate SYN LUBE 22 PAO-Based Multi-Purpose Synthetic Fluid

WCON5444 / 198697

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.