MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NeoGraf GRAFOIL® TG679 Expanded Natural Graphite Powder
Categories: Carbon; Graphite

Material Notes: GRAFOIL® Grade TG679 is an expanded natural graphite powder with consistent purity and good lubrication properties. Typical applications include using the graphite powder as an electrically conductive additive or as a thermal transfer enhancement in plastics and foams or as a lubricant. GRAFOIL® Grade TG679 has Nano particle-like properties at the macro particle pricing level.

Formerly a product of GrafTech.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0620 g/cc0.00224 lb/in³A.D. (Scott)
Moisture Absorption at Equilibrium 0.30 %0.30 %0.5% max
Particle Size 2.5 µm2.5 µmTypical Particle Thickness
Specific Surface Area 20 m²/g20 m²/g
Ash 2.5 %2.5 %3.5% max
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.10 %0.10 %
Barium, Ba 0.00040 %0.00040 %
Calcium, Ca 0.26 %0.26 %
Chromium, Cr 0.00040 %0.00040 %
Copper, Cu 0.00090 %0.00090 %
Iron, Fe 0.21 %0.21 %
Magnesium, Mg 0.16 %0.16 %
Manganese, Mn 0.0016 %0.0016 %
Molybdenum, Mo 0.0012 %0.0012 %
Silicon, Si 0.50 %0.50 %
Sulfur, S 0.050 %0.050 %
Titanium, Ti 0.0070 %0.0070 %
Vanadium, V 0.00050 %0.00050 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Diamond, Natural
Goodfellow CVD Graphene Film on Copper Foil
Graphite, Carbon, C
Tetracalcium-Phosphate, Ca4PO9
Aremco Graphi-Bond™ 551-R

CGRAF945 / 107349

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.