MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Henkel Loctite® Ultra Grey® 5999 Flange Sealant
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes:
Silicone Gasketing
Loctite® Silicone Gasketing materials include unique products with excellent resistance, formulations for high operating temperatures, and UV-curing formulations for cure-in-place production requirements. Silicone gasketing products are best suited for large gap applications and stamped metal assemblies where flexing occurs.

Loctite® 5999 Form-in-place Heavy Body RTV Silicone Ultra Grey® Flange Sealant
High modulus for rigid flange assemblies. Heavy body provides instant seal. Excellent oil, transmission fluid, gear oil, and water/glycol resistance. Non-corrosive. Low odor. Low volatility. Grey. Cure Type: Moisture Typical Use: Oil/water resistant, instant seal

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.45 g/cc0.0524 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060
Tensile Strength, Ultimate 3.45 MPa500 psi
Elongation at Break 175 %175 %
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C400 °F
Minimum Service Temperature, Air -53.9 °C-65.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min24.0 hourFull Cure; Varies with substrates
Tack-Free Time 10.0 min0.167 hour
 
Descriptive Properties
ColorGrey
Extrusion Rate105 g/min
Gap Fill0.24 in.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Henkel Loctite® Ultra Grey® 5699 Flange Sealant
Master Bond Supreme 11HT High Temperature Resistant Two Component Epoxy System
Master Bond Supreme 33 High Temperature Resistant, Structural Adhesive
Master Bond Supreme 11HT-LO Adhesive and Sealant Serviceable to +400°F
Master Bond EP21TDCF-3 Two Component, Higher Viscosity Epoxy System

PLOCT142 / 51878

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.