MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Shandong Dongyue Polymer DF-302 PTFE Aqueous Dispersion 60%
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Usage: The resin is used for impregnating porous material, such as asbestos, fiberglass, anti-corrosive, abrasion resistant, filature and lubricating materials.

Packing: The PTFE is packed in PVC circular barrels.

Transportation: The products are transported according to non-dangerous products. Heat, moisture, freezing and strong shock should be avoided during transportation. Over-bumpiness is apt to make the resin settle down.

Conformable with Q/DYG 005-2003

Information provided by Shandong Dongyue Polymer Material Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
pH 7.0 - 8.07.0 - 8.0
Viscosity 15 - 30 cP15 - 30 cP
 
Descriptive Properties
AppearanceMilky or Yellowish liquid
Content of Case Active Agent (%)4-6
For Processcoating and impregnating
PTFE Content (%)58-62

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Shandong Dongyue Polymer DF-301 PTFE Aqueous Dispersion 60%
Daikin PTFE D-210 DISPERSION Polytetrafluoroethylene Aqueous Dispersion
AGC Fluon® PTFE
AGC Fluon® AD639 PTFE Aqueous Dispersion
AGC Fluon® AD1 PTFE Aqueous Dispersion

PSHADP11 / 103662

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.