Injection molding grade. Nylene 401 is recommended for general purpose nylon molding applications in both thin and heavy sections. Nylene 401 has high flow characteristics at minimal processing temperatures.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |