MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Armstrong A-12-T Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Provides the same basic properties as A-12, but in thixotropic, non-sag, easily-brushable paste form. An ideal material for use where adhesive flow during cure cannot be tolerated. A-12-T meets the requirements of Mil. Spec. MIL-A-47074 (MIL) Type II, Class 2.

Information provided by Ellsworth Adhesives.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080
Tensile Strength, Ultimate 35.2 MPa5100 psiafter optimum cure
Elongation at Break 1.8 %1.8 %
Adhesive Bond Strength 45.5 MPa6600 psiSteel-Steel; after optimum cure
 14.8 MPa
@Temperature 82.2 °C
2150 psi
@Temperature 180 °F
Aluminum-Aluminum tensile shear
 22.1 MPa
@Temperature -54.4 °C
3200 psi
@Temperature -66.0 °F
Aluminum-Aluminum tensile shear
 32.8 MPa
@Temperature 25.0 °C
4750 psi
@Temperature 77.0 °F
Aluminum-Aluminum tensile shear
 
Thermal PropertiesMetricEnglishComments
CTE, linear 31.0 µm/m-°C
@Temperature 20.0 °C
17.2 µin/in-°F
@Temperature 68.0 °F
Glass Transition Temp, Tg 62.0 °C144 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 22.2 °C72.0 °F
 73.9 °C165 °FOptimum cure is 2 hr. @ 165°F
 149 °C300 °FFast cure is 5 min. @ 300°F
Pot Life <= 90.0 min
@Temperature 25.0 °C
<= 90.0 min
@Temperature 77.0 °F
100 g
 
Descriptive Properties
ColorBrown
Mix Ratio1/1By Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Armstrong A-12 Epoxy Adhesive, at 2:3 Mix Ratio
Armstrong A-12 Epoxy Adhesive, at 3:2 Mix Ratio
Armstrong A-12 Epoxy Adhesive, at 1:1 Mix Ratio
Morgan Advanced Ceramics GBC-92% Alumina 92-SV Aluminum Oxide Ceramic
CeramTec V 679 Alumina, 99.7%

PARM18 / 24550

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.