MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NHEP Spectron™ E5469 Nylon 66, 33% Glass Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Natural color. E5469 exhibits high rigidity, mechanical strength, and excellent appearance. It is suitable for wide range of applications.

Property data measured at room temperature, 50% RH.

Information provided by Bieglo Gmbh for Ngai Hing Engineering Plastic (Hong Kong) Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 165 MPa23900 psiASTM D638
Elongation at Yield 7.0 %7.0 %ASTM D638
Flexural Strength 220 MPa31900 psiASTM D790
Flexural Modulus 8.40 GPa1220 ksiASTM D790
Izod Impact, Notched 0.800 J/cm1.50 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 240 °C464 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 235 - 245 °C455 - 473 °F
Middle Barrel Temperature 245 - 255 °C473 - 491 °F
Front Barrel Temperature 255 - 265 °C491 - 509 °F
Nozzle Temperature 265 - 275 °C509 - 527 °F
Mold Temperature 90.0 - 120 °C194 - 248 °F
Drying Temperature 100 - 120 °C
@Time 7200 - 14400 sec
212 - 248 °F
@Time 2.00 - 4.00 hour
 
Descriptive Properties
Processing Injection PressureMedium-High
Processing Injection SpeedMedium-High

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NHEP Spectron™ E6666 Nylon 66, 30% Glass Fiber
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Unitika P-3001S Engineering Plastic
Unitika P-3001 Engineering Plastic
Unitika U-100 Engineering Plastic

PNGAI900 / 150495

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.