MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Videolar-Innova 500 Crystal Polystyrene (GPPS)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Transparent Grade

Material Notes:
  • Designed for injection molding
  • Very easy flowing grade for fast cycle injection molding
  • Excellent processability for filling thin parts
Features:
  • Good strength
  • Good temperature resistance
  • Excellent clarity
Applications:
  • Electronics packaging and office accessories
  • Coextrusion for laminates and film

Information provided by Dax Resinas

Key Words: FDA 21 CFR 177.1640
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.650 g/cc0.0235 lb/in³ISO 060
Density 1.04 g/cc0.0376 lb/in³ASTM D792
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm0.0030 - 0.0060 in/in
Melt Flow 16 g/10 min
@Load 5.00 kg,
Temperature 200 °C
16 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 42.0 MPa6090 psiASTM D638
Tensile Modulus 2.62 GPa380 ksiASTM D638
Flexural Strength 76.0 MPa11000 psiASTM D790
Flexural Modulus 3.17 GPa460 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 93.0 °C199 °F@ 264 psi; ASTM D648
Vicat Softening Point 98.0 °C208 °FASTM D1525
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
I. Stern GPPS-004 General Purpose Crystal Polystyrene
A. Schulman Diamond GPPS BEADS Injection Molding Grade, General Purpose Polystyrene
Chevron Phillips MC3650 Crystal Polystyrene
LG Chemical GPPS 15NF(I) PS, High Transparency, Heat Resistance
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded

PDAX002 / 29427

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.