MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Axiall HF-6597 Rigid PVC, Molding  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Georgia Gulf HF-6597 is a high flow PVC compound designed for thin wall parts and multi-cavity molds. It is ideally suited for a variety of electrical and appliance applications.

Information provided by Georgia Gulf

Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.34 g/cc1.34 g/ccASTM D-792
Linear Mold Shrinkage 0.0030 - 0.0040 cm/cm0.0030 - 0.0040 in/inASTM D-955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9797ASTM D-785
Tensile Strength at Break 36.42 MPa5282 psiASTM D-638
Tensile Strength, Yield 41.4 MPa6000 psiASTM D-638
Elongation at Break 139.2 %139.2 %ASTM D-638
Tensile Modulus 2.69 GPa390 ksiASTM D-638
Flexural Strength 67.6 MPa9800 psiASTM D-790
Flexural Modulus 2.48 GPa360 ksiASTM D-790
Izod Impact, Notched  0.801 J/cm
@Thickness 3.17 mm,
Temperature -20.0 °C
1.50 ft-lb/in
@Thickness 0.125 in,
Temperature -4.00 °F
ASTM D-256
 8.01 J/cm
@Thickness 3.17 mm,
Temperature 23.0 °C
15.0 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Gardner Impact 14.7 J
@Temperature 23.0 °C
10.8 ft-lb
@Temperature 73.4 °F
1/2" R Tup, 65 mil
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 72.00 °C161.6 °FASTM D-648
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C158 °FASTM D-648
UL RTI, Electrical 90.0 °C
@Thickness 1.50 mm
194 °F
@Thickness 0.0591 in
UL-746B
UL RTI, Mechanical with Impact 85.0 °C
@Thickness 1.50 mm
185 °F
@Thickness 0.0591 in
UL-746B
UL RTI, Mechanical without Impact 90.0 °C
@Thickness 1.50 mm
194 °F
@Thickness 0.0591 in
UL-746B
Flammability, UL94 5VA5VA
Oxygen Index 36 %36 %ASTM D-2863
 
Descriptive Properties
Flow Ratio (Distance/Wall Thickness, 390-400°F)230Georgia Gulf Test
UL Weatherability Rating F(1)UL-746C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Geon® Performance Solutions Vinyl Rigid Molding M5240 Polyvinyl Chloride, Rigid
Envalior Pocan® AF 4130 000000 PBT, 30% Glass Fiber Reinforced
Axiall 6680 Rigid PVC, Molding, White 476
Domo TechnylStar™ S 60G1 V30 PA6, 30% glass filled, DRY
Envalior Pocan® BF 4130 XF 000000 PBT, 30% Glass Fiber

PGGUL477 / 41753

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.