MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LNP Lexan® SML5877 Polycarbonate  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes:
  • Features: Low Viscosity, Antistatic
  • Forms: Pellets
  • Processing Method: Injection Molding

Information provided by LNP, a GE Plastics Company.

This data sheet is labeled Discontinued; however many LNP grades are still active under new names instituted after the SABIC purchase.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 62.1 MPa9010 psiType I, 50 mm/min; ASTM D638
Tensile Strength, Yield 71.0 MPa10300 psiType I, 50 mm/min; ASTM D638
Elongation at Break 100 %100 %Type I, 50 mm/min; ASTM D638
Elongation at Yield 5.8 %5.8 %Type I, 50 mm/min; ASTM D638
Tensile Modulus 2.70 GPa392 ksi50 mm/min; ASTM D638
Flexural Yield Strength 114 MPa16500 psi(50.8 mm Span) 1mm/min; ASTM D790
Flexural Modulus 2.76 GPa400 ksi(50.8 mm Span) 1mm/min; ASTM D790
Izod Impact, Notched 0.480 J/cm0.899 ft-lb/inASTM D256
Falling Dart Impact 74.6 J55.0 ft-lbASTM D3763
 75.9 J
@Temperature -40.0 °C
56.0 ft-lb
@Temperature -40.0 °F
ASTM D3763
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+13 ohm1.00e+13 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
@Thickness 3.18 mm
219 °F
@Thickness 0.125 in
Unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 260 - 282 °C500 - 540 °F
Middle Barrel Temperature 271 - 293 °C520 - 559 °F
Front Barrel Temperature 282 - 304 °C540 - 579 °F
Nozzle Temperature 277 - 299 °C531 - 570 °F
Melt Temperature 282 - 304 °C540 - 579 °F
Mold Temperature 71.1 - 93.3 °C160 - 200 °F
Drying Temperature 121 °C250 °F
Dry Time 3 - 48 hour3 - 48 hour
Moisture Content 0.020 %0.020 %Suggested
Back Pressure 0.345 - 0.689 MPa50.0 - 99.9 psi
Clamp Pressure 41.0 - 69.0 MPa5950 - 10000 psi
Shot Size 40 - 60 %40 - 60 %Suggested
Vent Depth 0.00250 - 0.00760 cm0.000984 - 0.00299 in
Screw Speed 40 - 70 rpm40 - 70 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo CALIBRE™ 603 5 Polycarbonate, Branched
Trinseo CALIBRE™ 200-15 Polycarbonate, General Purpose
LNP Lexan® SML5870 Acrylonitrile Butadiene Styrene + PC Alloy
LNP Lexan® SML5790 Polycarbonate, 10% Glass Fiber Reinforced
LNP Lexan® LG1500 Polycarbonate

PZLNP1115 / 51197

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.