MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow VORANOL™ 4815 Polyether Polyol
Categories: Polymer; Thermoset

Material Notes: VORANOL™ 4815 polyether polyol is a high reactivity capped triol. Its high molecular weight and high primary hydroxyl content make it well suited for high resiliency, flexible molded foams.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.017 g/cc1.017 g/cc
pH 8.88.8(1 Water / 10 Methanol)
Viscosity Measure  86 cSt
@Temperature 98.9 °C
86 cSt
@Temperature 210 °F
 680 cSt
@Temperature 37.8 °C
680 cSt
@Temperature 100 °F
 1180 cSt
@Temperature 25.0 °C
1180 cSt
@Temperature 77.0 °F
Maximum Moisture Content 0.0600.060wt% water
ASTM Color <= 50<= 50APHA
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 0.0200.020[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 224 °C>= 435 °F
 
Descriptive Properties
Hydroxyl Number mg KOH/g28.1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow VORANOL™ 4701 Polyether Polyol
Dow VORANOL™ 4240 Polyether Polyol
Dow VORANOL™ 4701C Polyether Polyol
Dow VORANOL™ 4703 Polyether Polyol
Dow VORANOL™ CP 4711 Polyol

PDOW1473 / 30691

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.