MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Omni Plastics OmniCarb™ PC/PBT 400IM2 UV PC/PBT Alloy
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced

Material Notes: Cold temperature impact resistant, UV stabilized; values are based on natural or black materials unless otherwise noted.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc1.18 g/ccASTM D792
Linear Mold Shrinkage 0.0050 - 0.011 cm/cm0.0050 - 0.011 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0050 - 0.010 cm/cm0.0050 - 0.010 in/inASTM D955
Melt Flow 12 g/10 min12 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 52.0 MPa7540 psiASTM D638
Elongation at Break 120 %120 %ASTM D638
Flexural Strength 83.0 MPa12000 psiASTM D790
Flexural Modulus 1.931 GPa280.1 ksiASTM D790
Izod Impact, Notched  6.41 J/cm
@Thickness 3.17 mm,
Temperature -30.0 °C
12.0 ft-lb/in
@Thickness 0.125 in,
Temperature -22.0 °F
ASTM D256
 7.57 J/cm
@Thickness 3.17 mm,
Temperature 22.8 °C
14.2 ft-lb/in
@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 96.0 °C
@Thickness 3.17 mm
205 °F
@Thickness 0.125 in
ASTM D648
Flammability, UL94  HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
Black color only
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0590 in
Black color only
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 227 - 243 °C440 - 470 °F
Middle Barrel Temperature 232 - 249 °C450 - 480 °F
Front Barrel Temperature 238 - 260 °C460 - 500 °F
Nozzle Temperature 238 - 260 °C460 - 500 °F
Melt Temperature 238 - 260 °C460 - 500 °F
Mold Temperature 48.9 - 82.2 °C120 - 180 °F
Drying Temperature 104 - 116 °C220 - 240 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Moisture Content <= 0.020 %<= 0.020 %
Back Pressure 0.345 - 0.689 MPa50.0 - 100 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Techmer ES Plastiblend® PC/PBT IM 1799 BK
MRC Polymers NAXALOY™ 780 PC+PBT Polyester Blend
Omni Plastics OmniCarb™ PC/PBT 1320 CTI PC/PBT
Omni Plastics OmniCarb™ PC/PBT 400IM2 PC/PBT Alloy
Techmer ES Plastiblend® PC/PBT IM 1012

POMNI5123 / 185269

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.