MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Crelan® NW 5 Polyurethane Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Thermoset; Polyurethane, TS

Material Notes: Crelan NW 5 is a blocked cycloaliphatic polyisocyanate. It is suitable as a hardener for polyurethane powder coatings.

Properties / Applications: Coatings based on Crelan NW 5 are characterized by their excellent flow properties and high gloss values. Depending on the polyester used, excellent gloss retention and chalking resistance in outdoor weathering can be obtained. As powder coatings based on Crelan NW 5 also provide good corrosion protection properties, they are ideal for use in outdoor applications. Crelan NW 5 is a hardener for hydroxyl-bearing polyesters based on Desmodur W. A NCO : OH ratio of 1.0 is recommended for optimum film properties. Slight undercrosslinking (NCO : OH ratio = 0.9) is possible depending on the co-reactants used and the film properties required. Overcrosslinking produces no advantages. As with any product, use of Crelan NW 5 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 100 - 250 cP100 - 250 cP
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 48.0 - 58.0 °C118 - 136 °F
 
Descriptive Properties
Color<100Hazen, 55% in toluene
Content<0.5%Monomeric diisocyanate
 <1.5%Non-blocked NCO
 12.7%Total NCO

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lord Adhesives Chemglaze® V004 Polyurethane Coating
General Plastics LAST-A-FOAM® FR-7140 Polyurethane Foam
Sawbones Solid Rigid Polyurethane Foam 15 pcf Density
Lord Adhesives Chemglaze® V175 Polyurethane Coating
Socomore Chemglaze® V300 Polyurethane Coating

PCOVEST0275 / 202058

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.