MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis BorSafe™ ME3441 Yellow Medium Density Polyethylene for Natural Gas Pipes
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Extruded

Material Notes: ME3441 is a yellow, bimodal, cadmium free, medium density polyethylene compound classified as a MRS 8.0 material (PE80) produced with the advanced Borstar technology. It includes a combination of pigments and stabilizers to ensure excellent long-term thermal stability and UV-resistance and resistance to gas condensate. It also shows excellent resistance to rapid crack propagation and slow crack growth.

ME3441 is recommended for pressure pipe systems in the application fields of rapid crack propagation and slow crack growth. Thanks to the structure, it gives outstanding extrudability, compared to conventional PE80 products.

Former trade name for this product was Borstar®.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.944 g/cc0.0341 lb/in³ISO 1183
Environmental Stress Crack Resistance >= 2000 hour
@Temperature 80.0 °C
>= 2000 hour
@Temperature 176 °F
At 8 bar; ISO 13479
Melt Flow 0.80 g/10 min
@Load 5.00 kg,
Temperature 190 °C
0.80 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 19.00 MPa2755 psiAt 50 mm/min; ISO 527-2
Elongation at Break >= 600 %>= 600 %ISO 527-2
Tensile Modulus 0.800 GPa116 ksiAt 1 mm/min; ISO 527-2
 
Processing PropertiesMetricEnglishComments
Front Barrel Temperature 180 - 210 °C356 - 410 °F
Die Temperature 200 - 210 °C392 - 410 °F
Melt Temperature 200 - 220 °C392 - 428 °F
Head Temperature 200 - 210 °C392 - 410 °F
 
Descriptive Properties
Resistance to Rapid Crack Propagation, BAR7ISO 13477, Pc at 0°C, S4 / pipe size 250 mm SDR 11

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis BorSafe™ HE3470-LS Black HDPE Compound for Pressure Pipes
Borealis BorSafe™ ME3440 Black Medium Density Polyethylene for Pressure Pipes
Hippe PA 11 Nylon 11
Hippe PA 12 Nylon 12
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade

PBOREA134 / 27441

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.