MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AISI E4340 Steel, quenched 845°C, 315°C (600°F) temper
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 4000 Series Steel; Low Alloy Steel; Carbon Steel; Medium Carbon Steel

Material Notes: AISI E4340 has a favorable response to heat treatment (usually oil quenching followed by tempering) and exhibits a good combination of ductility and strength when treated thusly. Uses include piston pins, bearings, ordnance, gears, dies, and pressure vessels.

Key Words: alloy steels, UNS G43406, ASTM A304, ASTM A331, ASTM A505, ASTM A519
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.85 g/cc0.284 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 506506Converted from Rockwell C hardness.
Hardness, Rockwell C 4848
Hardness, Vickers 487487Converted from Rockwell C hardness.
Modulus of Elasticity 200 GPa29000 ksiAISI 4340
Bulk Modulus 159 GPa23100 ksiEstimated from elastic modulus
Poissons Ratio 0.290.29Typical for steel
Machinability 50 %50 %annealed and cold drawn. Based on 100% machinability for AISI 1212 steel.
Shear Modulus 78.0 GPa11300 ksiEstimated from elastic modulus
Charpy Impact  14.0 J
@Temperature -185 °C
10.3 ft-lb
@Temperature -301 °F
 19.0 J
@Temperature -130 °C
14.0 ft-lb
@Temperature -202 °F
 20.0 J
@Temperature -73.0 °C
14.8 ft-lb
@Temperature -99.4 °F
 20.0 J
@Temperature -18.0 °C
14.8 ft-lb
@Temperature -0.400 °F
 22.0 J
@Temperature 38.0 °C
16.2 ft-lb
@Temperature 100 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.0000248 ohm-cm
@Temperature 20.0 °C
0.0000248 ohm-cm
@Temperature 68.0 °F
 0.0000298 ohm-cm
@Temperature 100 °C
0.0000298 ohm-cm
@Temperature 212 °F
 0.0000552 ohm-cm
@Temperature 400 °C
0.0000552 ohm-cm
@Temperature 752 °F
 0.0000797 ohm-cm
@Temperature 600 °C
0.0000797 ohm-cm
@Temperature 1110 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.3 µm/m-°C
@Temperature 20.0 °C
6.28 µin/in-°F
@Temperature 68.0 °F
 12.4 µm/m-°C
@Temperature 250 °C
6.89 µin/in-°F
@Temperature 482 °F
 13.7 µm/m-°C
@Temperature 500 °C
7.61 µin/in-°F
@Temperature 932 °F
Specific Heat Capacity 0.475 J/g-°C0.114 BTU/lb-°FTypical 4000 series steel
Thermal Conductivity 44.5 W/m-K309 BTU-in/hr-ft²-°FTypical steel
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.38 - 0.43 %0.38 - 0.43 %
Chromium, Cr 0.70 - 0.90 %0.70 - 0.90 %
Iron, Fe 95.175 - 96.27 %95.175 - 96.27 %As remainder
Manganese, Mn 0.65 - 0.85 %0.65 - 0.85 %
Molybdenum, Mo 0.20 - 0.30 %0.20 - 0.30 %
Nickel, Ni 1.65 - 2.0 %1.65 - 2.0 %
Phosphorus, P <= 0.025 %<= 0.025 %
Silicon, Si 0.15 - 0.30 %0.15 - 0.30 %
Sulfur, S <= 0.020 %<= 0.020 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 4140 Steel, normalized at 870°C (1600°F), reheated to 845°C (1550°F), oil quenched, 260°C (500°F) temper, 25 mm (1 in.) round
AISI 4140 Steel, normalized at 870°C (1600°F), reheated to 845°C (1550°F), oil quenched, 315°C (600°F) temper, 25 mm (1 in.) round
AISI 4140 Steel, normalized at 870°C (1600°F), reheated to 845°C (1550°F), oil quenched, 370°C (700°F) temper, 25 mm (1 in.) round
AISI 4140 Steel, normalized at 870°C (1600°F), reheated to 845°C (1550°F), oil quenched, 595°C (1100°F) temper, 25 mm (1 in.) round
AISI 4140 Steel, normalized at 870°C (1600°F), reheated to 845°C (1550°F), oil quenched, 650°C (1200°F) temper, 25 mm (1 in.) round

M434DT / 7813

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.