MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Samyang Triel® 5300 Thermoplastic Polyether Ester Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester, TP; Polyether Ester Elastomer

Material Notes: TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor recreation equipments. TRIEL® can be processed by a variety of thermoplastic processing techniques like injection molding, extrusion and extrusion blow molding.

    Grade Characteristics:
  • Low modulus

Applications:

  • Specially suitable for injection molding of thin-walled parts & complicated molds which require high flow

All information provided by Samyang

Key Words: TPEE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccASTM D792
Water Absorption 0.50 %
@Time 86400 sec
0.50 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.012 - 0.013 cm/cm0.012 - 0.013 in/inASTM D955
Melt Flow 22 - 24 g/10 min
@Load 2.16 kg,
Temperature 230 °C
22 - 24 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 3535ASTM D2240
Tensile Stress at Strain  1.67 - 1.86 MPa
@Strain 5.0 %
242 - 270 psi
@Strain 5.0 %
ASTM D638
 3.53 - 3.73 MPa
@Strain 10 %
512 - 540 psi
@Strain 10 %
ASTM D638
 6.67 - 6.86 MPa
@Strain 50 %
967 - 996 psi
@Strain 50 %
ASTM D638
Elongation at Break >= 400 %>= 400 %ASTM D638
Flexural Yield Strength 2.94 MPa427 psiASTM D638
Flexural Modulus 0.0392 GPa5.69 ksiASTM D790
Izod Impact, Unnotched  NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
ASTM D256
 NB
@Temperature -23.0 °C
NB
@Temperature -9.40 °F
ASTM D256
Taber Abrasion, mg/1000 Cycles 3131CS-17 Wheel; ASTM D1044
 
Thermal PropertiesMetricEnglishComments
Melting Point 189 °C372 °FASTM D2117
Deflection Temperature at 0.46 MPa (66 psi) 54.0 °C129 °FRate B; ASTM D648
Vicat Softening Point 123 °C
@Load 1.02 kg
253 °F
@Load 2.25 lb
Rate B; ASTM D1525
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 170 - 220 °C338 - 428 °FInjection or Extrusion
Middle Barrel Temperature 180 - 220 °C356 - 428 °FInjection
 190 - 230 °C374 - 446 °FExtrusion
Front Barrel Temperature 180 - 220 °C356 - 428 °FInjection
 190 - 220 °C374 - 428 °FExtrusion
Nozzle Temperature 180 - 220 °C356 - 428 °FInjection
Die Temperature 190 - 220 °C374 - 428 °FExtrusion
Drying Temperature 80.0 - 90.0 °C176 - 194 °F
Dry Time 3 - 4 hour3 - 4 hour
Moisture Content <= 0.030 %<= 0.030 %
Injection Pressure 5.90 - 7.90 MPa856 - 1150 psi
Cycle Time - Injection 1.2 - 1.5 sec1.2 - 1.5 sec
Cycle Time - Cooling 10 - 20 sec10 - 20 sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Samyang Triel® 5400 Thermoplastic Polyether Ester Elastomer
Samyang Triel® 5407EF Thermoplastic Polyether Ester Elastomer
Samyang Triel® 5206SP Thermoplastics Polyetherester Elastomer, Double Extrusion
Samyang Triel® 5700(A) Thermoplastic Polyether Ester Elastomer
Chengdu Polyster H3030 Thermoplastic Polyether-ester Elastomer (TPEE)

PSAMY001 / 88083

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.