MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.5 PHR Sulfur
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced; Rubber or Thermoset Elastomer (TSE)

Material Notes: Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and many other high performance polyurethane applications. Like many oil resistant synthetic rubbers, Millathane 76 requires a treated grade of sulfur to ensure proper dispersion.

All information provided by TSE Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070
Tensile Strength 32.10 MPa4656 psi
Elongation at Break 546 %546 %
100% Modulus 3.98 MPa
@Strain 100 %
577 psi
@Strain 100 %
200% Modulus 8.943 MPa
@Strain 200 %
1297 psi
@Strain 200 %
300% Modulus 15.36 MPa
@Strain 300 %
2228 psi
@Strain 300 %
Tear Strength 58.8 kN/m336 pliDie C
Compression Set 58.8 %
@Temperature 70.0 °C,
Time 79200 sec
58.8 %
@Temperature 158 °F,
Time 22.0 hour
 
Processing PropertiesMetricEnglishComments
Cure Time 7.00 min
@Temperature 155 °C
0.117 hour
@Temperature 311 °F
TC90

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mearthane Durethane™ M DM-650A Foam Polyurethane
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber
Covestro Platilon® 2202 AC Polyurethane Film
Covestro Platilon® M2234 Polyether-Blockamide Film
Evonik VESTICOAT® UB 1174 Polyester-Polyurethane System

PMILL016 / 87060

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.