Physical Properties | Metric | English | Comments |
---|
Specific Gravity | 1.18 g/cc | 1.18 g/cc |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Shore A | >= 77 | >= 77 |
| 80 | 80 |
| 82 @Treatment Temp. 100 °C, Time 252000 sec | 82 @Treatment Temp. 212 °F, Time 70.0 hour |
| 82 @Treatment Temp. 100 °C, Time 605000 sec | 82 @Treatment Temp. 212 °F, Time 168 hour |
| 84 @Treatment Temp. 100 °C, Time 1.21e+6 sec | 84 @Treatment Temp. 212 °F, Time 336 hour |
| 84 @Treatment Temp. 100 °C, Time 3.60e+6 sec | 84 @Treatment Temp. 212 °F, Time 1000 hour |
Tensile Strength at Break | >= 24.58 MPa | >= 3565 psi |
| 25.13 MPa | 3645 psi |
| 21.62 MPa @Treatment Temp. 100 °C, Time 605000 sec | 3135 psi @Treatment Temp. 212 °F, Time 168 hour |
| 21.71 MPa @Treatment Temp. 100 °C, Time 1.21e+6 sec | 3149 psi @Treatment Temp. 212 °F, Time 336 hour |
| 21.89 MPa @Treatment Temp. 100 °C, Time 252000 sec | 3175 psi @Treatment Temp. 212 °F, Time 70.0 hour |
| 22.57 MPa @Treatment Temp. 100 °C, Time 3.60e+6 sec | 3273 psi @Treatment Temp. 212 °F, Time 1000 hour |
Tensile Stress at Strain | 1.97 MPa @Strain 25 % | 285 psi @Strain 25 % |
| >= 2.55 MPa @Strain 50 % | >= 370 psi @Strain 50 % |
| 2.62 MPa @Strain 50 % | 380 psi @Strain 50 % |
| >= 4.93 MPa @Strain 100 % | >= 715 psi @Strain 100 % |
| 5.07 MPa @Strain 100 % | 735 psi @Strain 100 % |
Elongation at Break | >= 290 % | >= 290 % |
| 295 % | 295 % |
| 185 % @Treatment Temp. 100 °C, Time 1.21e+6 sec | 185 % @Treatment Temp. 212 °F, Time 336 hour |
| 195.6 % @Treatment Temp. 100 °C, Time 3.60e+6 sec | 195.6 % @Treatment Temp. 212 °F, Time 1000 hour |
| 204 % @Treatment Temp. 100 °C, Time 605000 sec | 204 % @Treatment Temp. 212 °F, Time 168 hour |
| 206 % @Treatment Temp. 100 °C, Time 252000 sec | 206 % @Treatment Temp. 212 °F, Time 70.0 hour |
Modulus of Elasticity | 0.0138 GPa | 2.00 ksi |
Poissons Ratio | 0.49 | 0.49 |
Shear Modulus | 0.00462 GPa | 0.670 ksi |
Secant Modulus | 0.0131 GPa | 1.90 ksi |
Tear Strength Test | 570 | 570 |
Compression Set | 33 % @Temperature 100 °C, Time 79200 sec | 33 % @Temperature 212 °F, Time 22.0 hour |
| 37.5 % @Temperature 100 °C, Time 252000 sec | 37.5 % @Temperature 212 °F, Time 70.0 hour |
| 54 % @Temperature 100 °C, Time 1.21e+6 sec | 54 % @Temperature 212 °F, Time 336 hour |
|
Thermal Properties | Metric | English | Comments |
---|
Maximum Service Temperature, Air | 65.6 °C | 150 °F |
Glass Transition Temp, Tg | -18.3 °C | -1.00 °F |
|
Descriptive Properties |
---|
Strain Energy / Unit Volume at 20% Elongation (psi) | 36 |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding