MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Wacker Vinnapas® 315 Vinyl Acetate-Ethylene Copolymer
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Product description: VINNAPAS® 315 is a poly(vinyl alcohol) stabilized vinyl acetate-ethylene copolymer dispersion with a glass transition temperature (Tg) of +17 °C that offers high heat resistance and high tensile strength.

Properties: VINNAPAS® 315 is designed for use as a base for high-speed packaging adhesives. It exhibits very high wet tack and high thickening response. Because of its poly(vinyl alcohol) stabilization and excellent mechanical stability, this dispersion has clean machining and can be used in a variety of roll, extruder or spray applications. The formaldehyde content of this dispersion is very low as it is manufactured with chemicals that do not generate formaldehyde. The dry VINNAPAS® 315 film is tack-free and heatsealable. The higher Tg gives the dried adhesive film both very high heat resistance and high tensile strength while maintaining greater flexibility than poly(vinyl acetate) films. The initial adhesive strength is excellent and maintains this strength even after aging. VINNAPAS® 315 exhibits good water resistance and excellent plasticizer migration.

Application: VINNAPAS® 315 is an excellent base for adhesive formulators and can be used in a wide variety of applications. Its rapid setting speed is useful in carton, case forming, and sealing applications. The natural affinity of the dispersion to coated stocks as well as kraft and its good water resistance make this dispersion suitable for bag seams, cups, tube winding, and high pressure laminates. It can also be used for application areas which include but are not limited to bookbinding, padding, laminations of leather to cloth and fiberglass to paper, craft glues, microwave packaging, and envelope back gums.

Other Applications:

  • Rug Backing
  • Consumer Goods

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³
Solids Content 54 - 55 %54 - 55 %
Particle Size 1200 - 1800 µm1200 - 1800 µm
pH 4.0 - 5.04.0 - 5.0
Viscosity 1800 - 2700 cP1800 - 2700 cPdynamic
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 17.0 °C62.6 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Superwool® Plus Textiles Braided Packing Thermal Ceramic
Rogers Arlon LW201B##-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported)
Wacker Vinnol® H 40/60 Vinyl Chloride Copolymer
Wacker Vinnapas® 920 Vinyl Acetate-Ethylene Copolymer
Wacker Silres® BS OH 100 Silicone Masonry Water Repellent

PWACK9592 / 205121

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.