MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Goodfellow Aluminum-Lithium/SiC Metal Matrix Composite
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Aluminum Alloy

Material Notes: Information provided by Goodfellow.

Key Words: Silicon Carbide MMC, AlSiC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.62 g/cc0.0947 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 550 MPa79800 psiLongitudinal
Tensile Strength, Yield 500 MPa72500 psi
Elongation at Break 2.3 %2.3 %
Tensile Modulus 100 GPa14500 ksi
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 81 %81 %
Copper, Cu 1.2 %1.2 %
Lithium, Li 2.0 %2.0 %
Magnesium, Mg 0.80 %0.80 %
SiC 15 %15 %
 
Descriptive Properties
Volume Fraction SiC, %13

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum - SiC Metal Matrix Composite
M Cubed Technologies ABC-501 Aluminum alloy-50% B4C Metal Matrix Composite
Materion AlBeMet® AM 162 Rolled Sheet, Annealed
Materion AlBeCast™ IC910 Aluminum Beryllium Composite
Materion AlBeMet® AM 162 Extruded Bar, Annealed

NGOODF110 / 16194

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.