MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol Advanced Materials PEARLTHANE® 11T65D Thermoplastic Polyurethane Elastomer
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Type : Pearlthane® 11T65D is a polycaprolactone copolyester-based thermoplastic polyurethane.

Main Application : Injection Moulding

Special Features : Combining very high hardness with excellent mechanical properties.

All information provided by Merquinsa

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccISO 868
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6464ISO 2781
Tensile Strength, Yield 35.00 MPa5076 psiISO 527-2/5A/500
Elongation at Break 440 %440 %ISO 527-2/5A/500
50% Modulus 19.0 MPa
@Strain 50 %
19.0 MPa
@Strain 50 %
ISO 527-2/5A/500
100% Modulus 25.01 MPa
@Strain 100 %
3628 psi
@Strain 100 %
ISO 527-2/5A/500
300% Modulus 31.00 MPa
@Strain 300 %
4496 psi
@Strain 300 %
ISO 527-2/5A/500
Tear Strength 210 kN/m1200 pliISO 34-1B
Abrasion 2525loss (mm³); ISO 4649-A
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 144 °C291 °FISO 306
 
Processing PropertiesMetricEnglishComments
Feed Temperature 40.0 °C104 °F
Nozzle Temperature 225 °C437 °F
Zone 1 220 °C428 °F
Zone 2 225 °C437 °F
Zone 3 230 °C446 °F
Zone 4 230 °C446 °F
Dry Time 3.00 hour
@Temperature 100 °C
3.00 hour
@Temperature 212 °F
Dew Point <= -30.0 °C<= -22.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Advanced Materials PEARLTHANE® 11T60D Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® 11H98 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® 15N95UV Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials Pearlthane® 11T85 Polycaprolactone Copolyester based TPU

PMES53 / 88430

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.