- Low swell
- Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a
UNIVAL™ DMDA-6320 NT 7 is a multipurpose polymer designed for the high speed production of blow molded containers used to package household industrial chemicals, toiletries and cosmetics, health and medicinal aids, and food products. In addition, it can be blow molded into other thin walled parts and houseware items and can be extruded into profiles. Information provided by Dow |