MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical LUPOY GN1006FL PC, Halogen Free, Flame Retardant, Transparency
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Unreinforced, Flame Retardant

Material Notes: Description: Injection Molding, PC, Halogen Free Flame Retardant, Transparency

Application: IT/OA, Electric & Electronic Housing and Components

CAS: 103598-77-2

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 g/cc1.21 g/ccASTM D792
Maximum Moisture Content 0.0200.020Injection Molding
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 22 g/10 min
@Load 1.20 kg,
Temperature 300 °C
22 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 118118ASTM D785
Tensile Strength, Yield 61.8 MPa
@Thickness 3.20 mm
8960 psi
@Thickness 0.126 in
50mm/min; ASTM D638
Elongation at Break >= 100 %
@Thickness 3.20 mm
>= 100 %
@Thickness 0.126 in
50mm/min; ASTM D638
Flexural Yield Strength 91.2 MPa
@Thickness 3.20 mm
13200 psi
@Thickness 0.126 in
10mm/min; ASTM D790
Flexural Modulus 2.26 GPa
@Thickness 3.20 mm
327 ksi
@Thickness 0.126 in
10mm/min; ASTM D790
Izod Impact, Notched >= 6.86 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
>= 12.9 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+15 ohm-cm2.00e+15 ohm-cmASTM D257
Arc Resistance 0.00 - 60 sec0.00 - 60 secASTM D495
Comparative Tracking Index 175 - 250 V175 - 250 V
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min3.15 - 5.91 in/min
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) >= 130 °C
@Thickness 6.40 mm
>= 266 °F
@Thickness 0.252 in
Unannealed; ASTM D648
Vicat Softening Point 141 °C
@Load 5.00 kg
286 °F
@Load 11.0 lb
50°C/h; ASTM D1525
UL RTI, Electrical  120 °C
@Thickness >=1.50 mm
248 °F
@Thickness >=0.0591 in
 120 °C
@Thickness >=2.00 mm
248 °F
@Thickness >=0.0787 in
 120 °C
@Thickness >=2.50 mm
248 °F
@Thickness >=0.0984 in
 120 °C
@Thickness >=3.00 mm
248 °F
@Thickness >=0.118 in
UL RTI, Mechanical with Impact  110 °C
@Thickness >=1.50 mm
230 °F
@Thickness >=0.0591 in
 110 °C
@Thickness >=2.00 mm
230 °F
@Thickness >=0.0787 in
 110 °C
@Thickness >=2.50 mm
230 °F
@Thickness >=0.0984 in
 110 °C
@Thickness >=3.00 mm
230 °F
@Thickness >=0.118 in
UL RTI, Mechanical without Impact  120 °C
@Thickness >=1.50 mm
248 °F
@Thickness >=0.0591 in
 120 °C
@Thickness >=2.00 mm
248 °F
@Thickness >=0.0787 in
 120 °C
@Thickness >=2.50 mm
248 °F
@Thickness >=0.0984 in
 120 °C
@Thickness >=3.00 mm
248 °F
@Thickness >=0.118 in
Flammability, UL94  V-2
@Thickness >=1.50 mm
V-2
@Thickness >=0.0591 in
 V-1
@Thickness >=2.00 mm
V-1
@Thickness >=0.0787 in
 V-0
@Thickness >=2.50 mm
V-0
@Thickness >=0.0984 in
 V-0
@Thickness >=3.00 mm
V-0
@Thickness >=0.118 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 260 - 280 °C500 - 536 °FInjection Molding
Middle Barrel Temperature 280 - 300 °C536 - 572 °FInjection Molding
Front Barrel Temperature 300 - 320 °C572 - 608 °FInjection Molding
Nozzle Temperature 300 - 320 °C572 - 608 °FInjection Molding
Melt Temperature 300 - 320 °C572 - 608 °FInjection Molding
Mold Temperature 80.0 - 120 °C176 - 248 °FInjection Molding
Drying Temperature 100 - 120 °C212 - 248 °FInjection Molding
Dry Time 3.00 - 5.00 hour3.00 - 5.00 hourInjection Molding
Back Pressure 0.981 - 3.92 MPa142 - 569 psiInjection Molding
Screw Speed 40 - 70 rpm40 - 70 rpmInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical HI855M PMMA, Impact Resistant Grade
LG Chemical AF342 ABS, Flame Retardant
LG Chemical LUPOY GN1002FL PC, Halogen Free, Flame Retardant, High Flow
LG Chemical ABS AF364 Injection Molding Grade
LG Chemical AF312A ABS, Flame Retardant

PLAY548 / 148558

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.