MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Meldin Supplier

DuPont Mobility and Materials Vespel® CP-9800 Carbon Fiber and Epoxy Composite, Ultra-high modulus end effectors
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Epoxy

Material Notes: Vespel® CP-9800 is a clean, stiff, light-weight new end effector material. Custom parts made from this pitch-based carbon fiber and epoxy composite are designed specifically for the function required in the application. CP-9800 raw material is produced in a sheet form with a maximum area of 1x2m and a thickness of 2-20mm.

This composite is ideally suited for flat panel display and wafer handling applications. When compared to traditional ceramic and aluminum end effectors, CP-9800 is lighter weight, more durable, and deflects less under equivalent load. These properties make Vespel® CP-9800 the ideal choice for your next robotic end effector application.

Applications: A pitch-based carbon fiber and epoxy composite for:

  • Flat panel displays
  • Wafer handling

Benefits:
  • Increase positional accuracy and dynamic performance
  • Stable transfer of large silicon wafers or LCD panels due to small deflection by self weight and loading
  • Reduce deflection and vibration without sacrificing stiffness

Information provided by DuPont. This product line has remained with DuPont after the DuPont-Dow merger.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.70 g/cc0.0614 lb/in³
Outgassing - Total Mass Loss 0.329 %0.329 %ASTM E595-93
Collected Volatile Condensable Material 0.0020 %0.0020 %ASTM E595-93
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 160 GPa23200 ksiLow Modulus
 200 GPa29000 ksiMedium Modulus
 250 GPa36300 ksiHigh Modulus
 320 GPa46400 ksiUltra High Modulus
Flexural Modulus 303 GPa44000 ksi
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 80.0 °C176 °FRegular Resin
 150 °C302 °FHeat Resistance-A Resin
 200 °C392 °FHeat Resistance-B Resin
 230 °C446 °FHeat Resistance-C Resin
 
Descriptive Properties
Deflection, mm0.19Wafer Handling; Case 2; Self Weight
 0.22Wafer Handling; Case 1; Loading by 12 in. wafer
 0.24Wafer Handling; Case 1; Self Weight
 0.3Loading
 0.47Wafer Handling; Case 2; Loading by 12 in. wafer
 0.48LCD Handling; Case 2; Self Weight
 0.62LCD Handling; Case 1; Self Weight
 0.8LCD Handling; Case 2; Loading by Plate Glass
 0.83Self Weight
 1.22LCD Handling; Case 1; Loading by Plate Glass
Finger Thickness, mm3
Finger Weight, kg0.24Wafer Handling; Case 2
 0.28Wafer Handling; Case 1
Finger weight, kg0.5
Hand Weight, kg1.2LCD Handling; Case 1
 2.9LCD Handling; Case 2
Resin Application Temperature, °C150Heat-Resistance-A
 200Heat-Resistance-B
 230Heat-Resistance-C
 80Regular

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Alcoa MIC-6 Aluminum Mold Alloy
Tungsten Carbide, WC
Aluminum 6061-T4; 6061-T451
Alclad Aluminum 6061-O
DuPont Mobility and Materials Vespel® CP-0644 Polyimide

PDU2051 / 32917

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.