MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polykemi AB SCANBLEND FS7 FR UV PC/ASA Blend, Flame-Retardant, UV Stabilized
Categories: Polymer; Thermoplastic; ASA Polymer; Polycarbonate (PC); Polycarbonate, Unreinforced, Flame Retardant; Polycarbonate/ASA Alloy, Unreinforced

Material Notes:

Information provided by Polykemi AB

Key Words: PC/ASA
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inISO 2577
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inISO 2577
Melt Index of Compound 35 g/10 min
@Load 5.00 kg,
Temperature 260 °C
35 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break <= 45.0 MPa<= 6530 psiISO/R527
Elongation at Yield 6.0 %6.0 %ISO/R527
Flexural Strength <= 80.0 MPa<= 11600 psiISO 178
Flexural Modulus 2.40 GPa
@Temperature 23.0 °C
348 ksi
@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched  3.50 J/cm²
@Temperature -20.0 °C
16.7 ft-lb/in²
@Temperature -4.00 °F
ISO 179
 4.00 J/cm²
@Temperature 23.0 °C
19.0 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C248 °F120°C/h; ISO 75/1
Deflection Temperature at 1.8 MPa (264 psi) 100 °C212 °F120°C/h; ISO 75/1
Vicat Softening Point  120 °C
@Load 5.001 kg
248 °F
@Load 11.03 lb
50°C/h; ISO 306
 135 °C
@Load 1.00 kg
275 °F
@Load 2.21 lb
50°C/h; ISO 306
Flammability, UL94 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
Glow Wire Test 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
IEC 695-2-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cossa Polimeri ESTABLEND PSA 8500 V0 HF Flame Retardant PC / ASA Blend
Omni Plastics OmniCarb™ PC/ASA 220 UV PC/ASA
Lotte Advanced Materials Infino® WX-7030 PC/ASA
Overview of materials for Polycarbonate, UV Stabilized
Polykemi AB SCANBLEND FS8 FR UV PC/ASA, Flame Retardant, UV-Stabilized

PPOLYK151 / 122876

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.