MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Scotchkote™ 206N Fusion Bonded Epoxy Coating (Fluid Bed Grade)
Categories: Polymer; Thermoset; Epoxy

Material Notes: 3M Scotchkote Fusion-Bonded Epoxy Coating 206N (Fluid Bed Grade) is a one-part, heat curable, thermosetting epoxy coating designed for corrosion protection of metal. The epoxy is applied to preheated steel as a dry powder which melts and cures to form a continuous, insulative corrosion barrier on pipe, fittings, valves, couplers, pumps and other equipment. Scotchkote coating 206N is NSF/ANSI 61 certified for potable water applications and is also resistant to corrosive soils, hydrocarbons, harsh chemicals and sea water.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.44 g/cc0.0520 lb/in³
Water Absorption <= 3.0 %<= 3.0 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 1818ASTM D2583
Tensile Strength at Break 26.9 MPa3900 psiASTM D2370
Elongation at Break 6.9 %6.9 %ASTM D2370
Compressive Strength 80.0 MPa11600 psiASTM D695
Gardner Impact 18.1 J13.3 ft-lb1.6 cm diameter tup, 0.32cm x 7.6cm x 7.6cm steel panel
Abrasion 0.1140.114[g] CS-17 1000g weight, 5000 cycles; ASTM D4060
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.30e+15 ohm-cm1.30e+15 ohm-cmASTM D257
Dielectric Strength 45.3 kV/mm1150 kV/inASTM D1000
 
Processing PropertiesMetricEnglishComments
Cure Time  3.00 min
@Temperature 246 °C
0.0500 hour
@Temperature 475 °F
 4.00 min
@Temperature 232 °C
0.0667 hour
@Temperature 450 °F
 6.00 min
@Temperature 218 °C
0.100 hour
@Temperature 424 °F
 10.0 min
@Temperature 204 °C
0.167 hour
@Temperature 399 °F
Gel Time  0.367 - 0.617 min
@Temperature 232 °C
0.367 - 0.617 min
@Temperature 450 °F
 0.6167 min
@Temperature 218 °C
0.6167 min
@Temperature 424 °F
 0.6667 min
@Temperature 204 °C
0.6667 min
@Temperature 399 °F
 2.40 min
@Temperature 246 °C
2.40 min
@Temperature 475 °F
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AppearanceBlue Green

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Scotchkote™ 206N XTRA LG Fusion Bonded Epoxy Coating
3M GM400 Gripping Material
Sorbothane Polyurethane Damping Material, 30 Durometer
DuPont Teijin Films Melinex® 357 Polyester Film
DSM Biomedical BioSpan® S SPU Segmented Polyether Polyurethane (SPU)

PMM35336 / 170083

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.