MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Axiall 7181 Rigid PVC, Extrusion  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Georgia Gulf 7181 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties:
  • Weatherability
  • Impact Strength
  • Dimensional Stability
  • Flame Retardant
  • Chemical Resistance

Information provided by Georgia Gulf

Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.42 g/cc1.42 g/ccASTM D-792
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm0.0020 - 0.0030 in/inASTM D-955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 112112ASTM D-785
Hardness, Shore D 8080ASTM D-2240
Tensile Strength, Yield 42.1 MPa6100 psiASTM D-638
Tensile Modulus 2.48 GPa360 ksiASTM D-638
Flexural Strength 75.8 MPa11000 psiASTM D-790
Flexural Modulus 2.83 GPa410 ksiASTM D-790
Izod Impact, Notched 9.61 J/cm18.0 ft-lb/inASTM D-256
Tensile Impact Strength 158 kJ/m²75.0 ft-lb/in²ASTM D-1822
Dart Drop Total Energy 53.4 J/cm0.100 ft-lb/mil23°C, C.125 Tup, Method A; ASTM D-4226
 
Thermal PropertiesMetricEnglishComments
CTE, linear 63.0 µm/m-°C
@Temperature 20.0 °C
35.0 µin/in-°F
@Temperature 68.0 °F
ASTM D-696
Deflection Temperature at 1.8 MPa (264 psi) 72.2 °C162 °FASTM D-648
Flammability, UL94 V-1V-1
 
Descriptive Properties
Cell Classification14413233ASTM D-4216
Color Values:?L=±1.0, ?a=±0.5, ?b=±0.5ASTM E-308/E-1345

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Axiall SP-7107 Rigid PVC, Molding
Axiall ProTherm® 4526 CPVC Rigid PVC, Molding
Axiall 7140 Rigid PVC, Extrusion & Molding
Axiall 6300 Rigid PVC, Molding

PGGUL412 / 41688

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.