MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Bamberger Polymers Bapolene® 4082NA Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Bapolene 4082NA is a homopolymer polypropylene designed for fast-cycle molding applications. It is nucleated and contains antistat . This product meets US FDA 21 CFR 177.1520.

Applications:

Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers

Key Words: Antistatic; Fast Molding Cycle; Food Contact Acceptable; Homopolymer; Nucleated.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D-1505
Melt Flow 35 g/10 min35 g/10 minASTM D-1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 37.9 MPa5500 psiASTM D-638
Flexural Modulus, 1% Secant 1690 MPa245000 psiASTM D-790A
Izod Impact, Notched 0.267 J/cm0.500 ft-lb/inASTM D-256
 
Compliance PropertiesMetricEnglishComments
FDA YesYesFDA 21 CFR 177.1520
 
Descriptive Properties
processInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bamberger Polymers Bapolene® 4062NA Polypropylene, Injection Grade
Bamberger Polymers Bapolene® 4062 Polypropylene, Injection Grade
LG Chemical SEETEC M1425 Polypropylene Impact Copolymer
LG Chemical SEETEC M1500 Polypropylene Impact Copolymer
Bamberger Polymers Bapolene® 222B Polyethylene Film Grade

PBP1122 / 90066

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.